EP30C

Two component, nickel filled epoxy for bonding, sealing and coating
Key Features
  • Good electrical and thermal conductivity
  • Excellent for EMI/RFI shielding
  • Reliable gap filling properties
  • Superior dimensional stability
Typical Properties
Viscosity
Paste
Cure Schedule
overnight at ambient temperatures followed by 1-2 hours at 150°F
Hardness
80-90 Shore D
Service Temperature Range
-60°F to +250°F
Coefficient of Thermal Expansion
25-30 X 10⁻⁶ in/in/°C
Thermal Conductivity
8-9 BTU•in/(ft²•hr•°F) [1.15-1.30 W/(m•K)]
Volume Resistivity
5-20 ohm-cm
Imagen
EP30C Two Part Epoxy
Certifications

Meets EU Directive 2015/863

Packaging
Product Description

Master Bond EP30C is a two component, nickel filled, electrically conductive epoxy for high performance bonding, sealing and coating. This system has a 100 to 4 mix ratio by weight, but unlike other nickel conductive epoxies, EP30C is a malleable type paste. It will fully cure at room temperature in 2-3 days, or at 150-200°F in 2-3 hours. The optimum cure schedule is overnight at ambient temperatures followed by 1-2 hours at 150°F.

EP30C has a good physical strength profile. It bonds well to a wide variety of substrates, including metals, composites, glass, ceramics, vulcanized rubbers and many plastics. For a conductive epoxy, It delivers above average strength performance. Most noteworthy are its compressive strength and tensile modulus. Also, it excels in being dimensionally stable and having low shrinkage upon cure. Its conductivity is useful for static dissipation, EMI/RFI shielding and grounding applications. Some other desirable attributes are good chemical resistance to water, oils and cleaning agents. The service temperature range is -60°F to +250°F. Part A is gray and Part B is clear. EP30C is particularly useful in aerospace, electronic, electrical and other industries where nickel conductivity is desirable from a functional and cost perspective.

Product Advantages

  • Mixed viscosity is a malleable paste
  • Versatile cure schedules; ambient temperature cures or fast elevated temperature cures as required
  • Electrically and thermally conductive
  • Better physical strength properties
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.