Most Popular Epoxy Compounds for the Oil and Gas Production Industry
Two component, toughened, quartz filled epoxy with exceptional abrasion resistance. Heat curing system. Long working life after mixing. High compressive strength. Superb dimensional stability. Serviceable from -60°F to +450°F. Withstands exposure to petrochemicals acids, bases, solvents. Good strength retention at elevated temperatures. Successfully tested for 1,000 at 85°C/85% RH.
Room temperature curing epoxy featuring excellent chemical resistance. 100% reactive. High bond strength. Fast cure speed. Withstands exposure to organic solvents. Convenient processing. Service temperature range -60°F to +250°F. Excellent electrical insulation properties.
Two component, ambient temperature curing system with excellent physical properties. Thermally stable. High compressive strength. Features extraordinary resistance to fuels, alcohols and organic solvents. Withstands 1,000 hours 85°C/85% RH. Service temperature range -60°F to +400°F. Moderate viscosity. Good electrical insulator.
One part, oven cured epoxy system with excellent thermal conductivity and superb resistance to thermal cycling. Primarily used for bonding of heat sinks and sensors where heat transfer is desirable. Serviceable from 4k to +400°F. Convenient processing.
High performance adhesive/sealant/coating. Serviceable from -80°F to +500°F. Resists thermal cycling. Outstanding resistance to acids, bases, petrochemicals, water. 100% reactive. Cures at elevated temperatures. Good flow properties. Moderate viscosity. Excellent performance profile for long term exposures at 400°F to 450°F. Well suited for moderate sized electronic potting applications.
Cures rapidly at moderate elevated temperatures. Superior resistance to moisture. Two part epoxy has long pot life at ambient temperatures. High bond strength properties. Reliable electrical insulator. Serviceable from -60°F to +450°F. Withstands aggressive chemical exposure. Tg 120-130°C. Shore D hardness >80.
Thermally conductive, electrically isolating epoxy serviceable from -60°F to +500°F. Heat curing, good flow. Superior chemical resistance properties. Long pot life. High compressive strength and dimensionally stable.