EP42HT-2AO-1 Black Two Part Epoxy
EP42HT-2AO-1 Black
Two part, room temperature curable epoxy adhesive, sealant, coating and casting system
Coefficient of Thermal Expansion
18-21 x 10⁻⁶ in/in/°C
Tensile Lap Shear Strength
900-1,100 psi
  • NASA Low Outgassing
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
  • Sealing
  • Coating
  • Casting
  • Encapsulation
  • Potting
Part A: 50,000-120,000 cps, Part B: 200-1,000 cps 75°F: 3-5 days; 200°F: 2-3 hours 85-90 Shore D 4K to +400°F /fr/tds/ep42ht-2ao-1-black
EP42HT-2FG Two Part Epoxy System
EP42HT-2FG
Two component epoxy system formulated for food applications
Tensile Modulus
>450,000 psi
Volume Resistivity
>10¹⁴ ohm-cm
  • FDA Food Grade 21 CFR 175.105
  • FDA Food Grade 21 CFR 175.300
  • RoHS Compliant
  • USP Class VI Medical
  • ISO 10993-5 for Cytotoxicity
  • Bonding
  • Sealing
  • Coating
  • Casting
  • Potting
  • Gap Filling
  • Encapsulation
Part A: 55,000-110,000 cps, Part B: 30-70 cps 150°-250°F for 3-4 hours; optimum cure schedule is overnight at 75°F followed by 3-4 hours at 150-250°F. >75 Shore D -60°F to +450°F /fr/tds/ep42ht-2fg
EP42HT-2FG Black Two Part Epoxy
EP42HT-2FG Black
Two component, high temperature resistant epoxy for indirect food applications
Dielectric Constant
4.6
Glass Transition Temperature (Tg)
145-150°C
  • FDA Food Grade 21 CFR 175.105
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Potting
  • Gap Filling
  • Casting
Part A: 55,000-110,000 cps, Part B: 30-80 cps overnight at 75°F followed by a post cure of 3-4 hours at 150-250°F 80-90 Shore D -60°F to +450°F /fr/tds/ep42ht-2fg-black
EP42HT-2LTE Two Component Epoxy Compound
EP42HT-2LTE
Two component, room temperature curing epoxy compound featuring an ultra low coefficient of thermal expansion
Coefficient of Thermal Expansion
9-12 X 10⁻⁶ in/in/°C
Dielectric Constant
4.4
  • 1,000 Hours at 85°C/85% RH
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gap Filling
paste cures within 4-7 days at 75°F; faster cures can be realized at elevated temperatures, e.g. hours at 150-200°F; desirable cure schedule is overnight at 75°F followed by 3-5 hours at 150-200°F 85-95 Shore D 4K to +300°F /fr/tds/ep42ht-2lte
EP42HT-2Med Two Part Epoxy System
EP42HT-2Med Black
Two component, high temperature resistant epoxy for medical device assembly
Dielectric Constant
4.0 at 75°F, 60Hz
Glass Transition Temperature (Tg)
150-155°C
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • USP Class VI Medical
  • Bonding
  • Sealing
  • Coating
  • Potting
  • Casting
  • Encapsulation
  • Gap Filling
Part A: 55,000-110,000 cps, Part B: 30-70 cps 48-72 hours at 75°F; 2-3 hours at 200°F 75-85 Shore D -60°F to +450°F /fr/tds/ep42ht-2med-black
EP42HT-2ND-2
Two component, room temperature curing epoxy compound featuring high temperature resistance
Dielectric Constant
4.4
Glass Transition Temperature (Tg)
150-155°C
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Paste 8-12 hours at 75°F followed by 2-4 hours at 175-250°F 80-90 Shore D -60°F to 450°F /fr/tds/ep42ht-2nd-2
EP42HT-2ND-2Med Black Two Part Epoxy System
EP42HT-2ND-2Med Black
Two component, high temperature resistant epoxy compound for medical device assembly
Dielectric Constant
4.0
Glass Transition Temperature (Tg)
150-155°C
  • ISO 10993-5 for Cytotoxicity
  • USP Class VI Medical
  • RoHS Compliant
  • Bonding
  • Sealing
  • Gap Filling
  • Coating
Part A: >1,000,000 cps, Part B: >250,000 cps overnight at 75°F followed by 6-8 hours at 135-165°F or 4-6 hours at 175-185°F 75-85 Shore D -60°F to +450°F /fr/tds/ep42ht-2nd-2med-black
EP42HT-3AO Two Part Epoxy
EP42HT-3AO
Two part, room temperature curable epoxy adhesive, sealant, coating and encapsulating system
Acoustical Impedance
5.3 MRayl
Glass Transition Temperature (Tg)
140-150°C
  • RoHS Compliant
  • NASA Low Outgassing
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gap Filling
  • Potting
40,000-80,000 cps Cure in 3-4 days at 75°F or 2-3 hours at 150-200°F; Recommended curing is overnight at 75°F followed by 2-3 hours at 150-200°F; Optimum cure schedule: Overnight at 75°F, followed by 2-3 hours at 150-200°F 85-95 Shore D 4K to +400°F /fr/tds/ep42ht-3ao
EP42HT-4AOMed Black Two Component Epoxy
EP42HT-4AOMed Black
Two part, thermally conductive epoxy for medical device manufacturing
Coefficient of Thermal Expansion
18-21 x 10⁻⁶ in/in/°C
Tensile Modulus
500,000-550,000 psi
  • RoHS Compliant
  • USP Class VI Medical
  • ISO 10993-5 for Cytotoxicity
  • 1,000 Hours at 85°C/85% RH
  • Bonding
  • Sealing
  • Coating
  • Casting
  • Encapsulation
  • Gap Filling
  • Potting
Part A: 50,000-120,000 cps, Part B: 200-1,000 cps overnight at 75°F, followed by 2-3 hours at 150-200°F 85-90 Shore D 4K to +400°F /fr/tds/ep42ht-4aomed-black
EP45HT Two Part Epoxy
EP45HT
Two component epoxy system for bonding, sealing, coating and encapsulation
Glass Transition Temperature (Tg)
150-160°C
Volume Resistivity
>10¹⁴ ohm-cm
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Casting
  • Encapsulation
  • Gap Filling
Part A: 60,000-110,000 cps, Part B: 500-2,500 cps 250°F for 3-4 hours or 300°F for 2-3 hours 75-85 Shore D -80°F to +500°F /fr/tds/ep45ht

Need Expert Guidance?

Our expert engineers offer one-on-one consultations to help you navigate our extensive material library and find the right solution for your application. We ensure confidentiality and quick turnaround (1-2 business days).