Product Selector

Filters
Applications
Product Type
Certifications
Thermal Conductivity
Product Certifications Applications Viscosity Cure Schedule Hardness Temp. Range Link to Content
EP51AO Two Part Epoxy
EP51AO
Two component, epoxy adhesive, sealant and coating compound
Coefficient of Thermal Expansion
25-30 x 10⁻⁶ in/in/°C
Dielectric Strength
>400 volts/mil
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Part A: 50,000-100,000 cps, Part B: 75,000-125,000 cps 75°F: 12-24 hours, 200°F: 1 hour >75 Shore D 4K to +250°F /fr/tds/ep51ao
EP53TC Two Part Epoxy
EP53TC
Two part epoxy with high thermal conductivity, electrically insulating, and low thermal resistance for bonding, sealing, coating, and potting
Acoustical Impedance
8.5 MRayl
Thermal Conductivity
16-18 BTU•in/(ft²•hr•°F) [2.31-2.60 W/(m•K)]
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Potting
  • Gap Filling
45,000-65,000 cps Cures at 80°C for 2 hours followed by 2-4 hours at 90-125°C. 85-95 Shore D -100°F to +300°F /fr/tds/ep53tc
EP54TC Two Part Epoxy
EP54TC
Two part epoxy with high thermal conductivity, electrically insulating, and low thermal resistance for bonding and sealing
Dielectric Constant
4.7
Thermal Conductivity
41.6-45.1 BTU•in/(ft²•hr•°F) [6.0-6.5 W/(m•K)]
  • RoHS Compliant
  • NASA Low Outgassing
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
100,000-200,000 cps 80°C for 2 hours followed by 2-4 hours at 90-125°C. An alternative cure schedule would be 4-6 hours at 80-90°C. 85-95 Shore D -100°F to +400°F /fr/tds/ep54tc
Two Part Epoxy EP54TCMed
EP54TCMed

Two part medical grade epoxy featuring exceptionally high thermal conductivity and electrical insulation, for bonding and sealing

Tensile Modulus
>1,000,000 psi
Thermal Conductivity
41.6-45.1 BTU•in/(ft²•hr•°F) [6.0-6.5 W/(m•K)]
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • Bonding
  • Sealing
100,000-200,000 cps The epoxy requires heat for curing. One option is 80°C for 2 hours followed by 2-4 hours at 90-125°C. An alternative cure schedule would be 4-6 hours at 80-90°C. 85-95 Shore D -100°F to +400°F [-73°C to +204°C] /fr/tds/ep54tcmed
EP5LTE-100 is a flowable, one part epoxy with a low coefficient of thermal expansion
EP5LTE-100
One component epoxy for bonding and sealing featuring a low coefficient of thermal expansion and a curing temperature of 100°C
Coefficient of Thermal Expansion
8-12 x 10⁻⁶ in/in/°C
Glass Transition Temperature (Tg)
120-125°C
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
20,000-160,000 cps 90-120 minutes at 100°C followed by 2-3 hours at 100-125°C 85-95 Shore D -76°F to +347°F /fr/tds/ep5lte-100
EP62-1 Two Part Epoxy System
EP62-1
Two component epoxy resin system featuring excellent temperature and chemical resistance
Dielectric Constant
4.2
Volume Resistivity
>10¹⁴ ohm-cm
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
4,000-8,000 cps 4-6 hours at 60-70°C, 20-40 minutes at 80-100°C or 10-20 minutes at 125°C 80-90 Shore D -60°F to +450°F /fr/tds/ep62-1
Two Component Epoxy EP62-1AO
EP62-1AO
Two component epoxy resin system featuring excellent temperature and chemical resistance
Dielectric Constant
4.8
Tensile Lap Shear Strength
800-1,000 psi
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste 4-6 hours at 140-160°F, 20-40 minutes at 175-200°F or 10-20 minutes at 250-300°F 80-90 Shore D -60°F to +450°F /fr/tds/ep62-1ao
EP62-1BF Two Component Epoxy
EP62-1BF
Two component, lower viscosity epoxy system featuring superior chemical resistance
Dielectric Constant
4.2
Volume Resistivity
>10¹⁴ ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Gap Filling
  • Coating
2,000-5,000 cps 6-8 hours at 140-158°F [60-70°C], 60-70 minutes at 176-212°F [80-100°C] or 20-30 minutes at 257°F [125°C] 80-90 Shore D -60°F to +400°F /fr/tds/ep62-1bf
EP62-1HT Two Part Epoxy
EP62-1HT
Two component, lower viscosity epoxy system featuring superior temperature and unsurpassed chemical resistance, especially to acids
Dielectric Constant
4.2 at 75°F, 60 Hz
Glass Transition Temperature (Tg)
145-155°C
  • RoHS Compliant
  • NASA Low Outgassing
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Part A: 55,000-110,000 cps, Part B: 100-1,000 cps 60-70 minutes at 176-212°F [80-100°C] or 20-30 minutes at 257°F [125°C] 80-90 Shore D -60°F to +450°F /fr/tds/ep62-1ht
Two Component Epoxy EP62-1HTMed
EP62-1HTMed
Two component epoxy with superior temperature and chemical resistance that withstands repeated and aggressive sterilization
Glass Transition Temperature (Tg)
145-155°C
Volume Resistivity
>10¹⁴ ohm-cm
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Part A: 55,000-110,000 cps, Part B: 100-1,000 cps 60-70 minutes at 176-212°F [80-100°C] or 20-30 minutes at 257°F [125°C] 80-90 Shore D -60°F to +450°F /fr/tds/ep62-1htmed