Thermally Conductive, Low Viscosity Epoxy Features Cryogenic Serviceability
Master Bond EP30FLAO is a two component epoxy resin system for high performance potting, bonding, sealing and coating. It is extremely versatile and can be used in a wide variety of cryogenic applications. This low viscosity epoxy with excellent flow characteristics makes it ideal as a thermally conductive potting compound. It is widely used in the electronic, electrical, computer, metalworking, appliance and chemical industries where electrical insulation, environmental protection and heat transfer is required.
EP30FLAO features a wide service temperature range of 4K to 250ºF. Its thermal conductivity is 9-10 BTU/in/ft²/hr/ºF. The viscosity of the mixed compound is 5,000 to 6,000 cps at 75ºF. In addition to these attractive attributes, it has a low thermal expansion coefficient, superior dimensional stability, good physical strength and toughness.
Parts A and B are available in half pint, pint, quart, one gallon and five gallon containers.
For Editorial Use
Click below to download this release in the format of your choice.
| צְרוּפָה | גודל |
|---|---|
| ep30flao_nr.doc (22 KB) | 22 KB |
| צְרוּפָה | גודל |
|---|---|
| ep30flao_nr.html (3.13 KB) | 3.13 KB |
| צְרוּפָה | גודל |
|---|---|
| ep30flao_nr.txt (2.4 KB) | 2.4 KB |
News Release Images
Click an image to download a high resolution version in JPEG format.