No Mix, Thermally Conductive, Electrically Insulative Epoxy System Cures Rapidly At 80°C
Developed for a variety of bonding, sealing, potting and encapsulation applications, Master Bond EP3RR-80 is a one component epoxy that offers user friendly handling. It has a moderate viscosity, good flow properties and an unlimited working life at ambient temperatures. Additionally, this system can be stored at 40-50°F and does not require freezing.
Unlike typical one part epoxies, EP3RR-80 will cure in 45-50 minutes at 80°C (175°F), or in 25-30 minutes at 250°F. It features low exotherm while curing enabling it to cure in thicker sections up to and beyond a 1/2 inch deep. This dimensionally stable compound forms high strength bonds to metals, composites, ceramics, glass and many plastics.
EP3RR-80 has superb electrical insulation characteristics and delivers a thermal conductivity of 5-6 BTU·in/(ft²•hr•°F) [0.72-0.87 W/(m•K)] at 75°F. Resistance to water, oils, fuels and many other chemicals is outstanding. Service operating temperature range is -100°F to +350°F.
This compound is widely employed in the electronic, aerospace, specialty OEM and related industries. It is available for use in syringes as well as standard containers ranging from ½ pints to gallons.
For Editorial Use
Click below to download this release in the format of your choice.
| צְרוּפָה | גודל |
|---|---|
| EP3RR-80_nr.doc (29 KB) | 29 KB |
| צְרוּפָה | גודל |
|---|---|
| EP3RR-80_nr.html (3.64 KB) | 3.64 KB |
| צְרוּפָה | גודל |
|---|---|
| EP3RR-80_nr.txt (2.77 KB) | 2.77 KB |
News Release Images
Click an image to download a high resolution version in JPEG format.