EP21TDCN-LO

Durable, two component epoxy for high performance bonding and sealing
Key Features
  • Convenient handling
  • Good electrical conductivity
  • Withstands thermal cycling
  • NASA low outgassing approved
Typical Properties
Viscosity
paste
Cure Schedule
Cures readily at 75°F in 3-4 days, or, alternatively, at 150-200°F for 2-3 hours. The optimum cure is overnight at 75°F, followed by 2-3 hours at 150-200°F.
Hardness
80-90 Shore D
Service Temperature Range
-100°F to +275°F
Tensile Lap Shear Strength
1,400-1,600 psi
Volume Resistivity
5-10 ohm-cm
תמונה
EP21TDCN-LO Two Part Epoxy System
Certifications

ASTM E595 Compliant

Meets EU Directive 2015/863

Packaging
Product Description

Master Bond EP21TDCN-LO is a two component, nickel filled, electrically conductive, adhesive for high performance bonding and sealing. Both Part A and Part B have smooth paste consistencies. The mix ratio is a forgiving one to one by either weight or volume. It cures readily at room temperature in 3-4 days, or, alternatively, at 150-200°F for 2-3 hours. The optimum cure is overnight at room temperature, followed by 2-3 hours at 150-200°F. The volume resistivity of the cured system is 5-10 ohm-cm. It is 100% reactive and does not contain any diluents or solvents.

Considering that it is an electrically conductive adhesive, EP21TDCN-LO has a reasonably good physical strength profile. It bonds well to metals, composites, ceramics and many plastics. Both Parts A and B are colored nickel. Most importantly, it is a toughened system, formulated to withstand relatively rigorous thermal cycling as well as mechanical vibration and shock. The service temperature range is -100°F to +275°F. It has good resistance to fuels, oils and water. EP21TDCN-LO is particularly effective for grounding and shielding applications. It is a good fit for a number of applications involving the aerospace, electronic and specialty OEM industries as well as vacuum and cleanroom applications where electrical conductivity and NASA low outgassing are desirable.

Product Advantages

  • Convenient mixing: one to one mix ratio by weight or volume
  • Cures at ambient or elevated temperatures
  • Good electrical and thermal conductivity, especially for grounding, shielding and static dissipation
  • Very good toughness; can hold up to thermal cycling
  • High bond strength to similar and dissimilar substrates
  • Contains no solvents or diluents
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.