Supreme 3HTND-2GT

One component, toughened epoxy adhesive, sealant, coating and glob top
Key Features
  • Excellent thermal conductivity
  • Fast curing
  • Withstands thermal cycling and shock
  • Serviceable from 100°F to +400°F
Typical Properties
Viscosity
paste
Cure Schedule
Cures in 20-30 minutes at 250°F or in 5-10 minutes at 300°F
Hardness
>75 Shore D
Service Temperature Range
-100°F to +400°F
Coefficient of Thermal Expansion
23-27 X 10⁻⁶ in/in/°C
Dielectric Constant
4.5
תמונה
Supreme 3HTND-2GT One Part Epoxy System
Certifications

Meets EU Directive 2015/863

Product Description

Master Bond Supreme 3HTND-2GT is a fast curing, toughened multifunctional one component high performance epoxy system that can be used for bonding, sealing, glob top and die attach applications. It has a huge array of highly desirable features, including no mixing, a convenient viscosity, sterling physical properties and very fast cures. Unlike many epoxies it can be readily and efficiently applied to a defined area. This epoxy combines excellent electrical insulation properties and thermal conductivity with top-notch dimensional stability and the capability of withstanding rigorous thermal cycling and shocks. It cures in 20-30 minutes at 250°F or in 5-10 minutes at 300°F with very low shrinkage. Supreme 3HTND-2GT can cure in thicknesses of up to 1/8 inch if needed. It bonds well to a wide variety of substrates used in electronics, including metals, composites, ceramics and many plastics. The service temperature range for this system is first rate at -100°F to +400°F. It resists chemicals rather well, including water, acids, bases and many solvents. Especially noteworthy, is its low level of ionic impurities. Supreme 3HTND-2GT is yellowish tan in color. As mentioned above, this multifaceted system can be used as a glob top or die attach and in other applications as an adhesive or sealant in electronics when the special combination of properties, particularly the limited flow characteristics when curing are desirable.

Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.