UV15X-6Med-2LV One Part UV Curable System
UV15X-6Med-2LV
UV system for high performance bonding, sealing and coating
Elongation
>100%
Refractive Index
1.50
  • RoHS Compliant
  • ISO 10993-5 for Cytotoxicity
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gap Filling
20,000-40,000 cps 10-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts/cm2 55-65 Shore D -80°F to +250°F /de/tds/uv15x-6med-2lv
UV15X-6NM-2 One Part UV Curable Epoxy Compound
UV15X-6NM-2
UV system for high performance bonding, sealing and coating
Elongation
>100%
Refractive Index
1.50
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
35,000-55,000 cps cures readily in 20-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts/cm2 25-45 Shore D -80°F to +250°F /de/tds/uv15x-6nm-2
UV Curable Adhesive System UV15X-6NM-2BCL
UV15X-6NM-2BCL
Blue colored UV system for high performance bonding, sealing and coating, turns clear upon exposure to UV light
Dielectric Constant
4.5
Refractive Index
1.50
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
35,000-55,000 cps UV light 320-365 nm for 30-60 seconds 25-45 Shore D -80°F to +250°F /de/tds/uv15x-6nm-2bcl
UV16 One Part UV Curable Compound
UV16
Low viscosity, one component, UV curable epoxy based system
Glass Transition Temperature (Tg)
95-100°C
Refractive Index
1.511
  • RoHS Compliant
  • NASA Low Outgassing
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
250-500 cps UV light 320-365 nm for 15-30 seconds 70-80 Shore D -80°F to +400°F /de/tds/uv16
UV16Med
Low viscosity, medical grade UV curable epoxy based system for bonding, sealing and coating
Dielectric Constant
3.1
Glass Transition Temperature (Tg)
90-95°C without post cure; 135-140°C with post cure.
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
250-500 cps UV light 320-365 nm for 20-30 seconds 70-80 Shore D. -80°F to +400°F. /de/tds/uv16med
UV16Med-FD One Part UV Curable Adhesive
UV16Med-FD

Low viscosity, medical grade UV curable epoxy for bonding, sealing and coating, contains a fluorescent dye for identification

Refractive Index
1.511
Tensile Modulus
250,000-300,000 psi
  • RoHS Compliant
  • ISO 10993-5 for Cytotoxicity
  • Bonding
  • Sealing
  • Coating
70-80 Shore D -80°F to +400°F /de/tds/uv16med-fd
UV17Med
UV system for high performance bonding, sealing and coating featuring superb adhesion to thermoplastic urethanes (TPUs)
Elongation
50-60%
Refractive Index
1.51
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
500-3,000 cps 10-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output of 20-40 milliwatts/cm2 65-75 Shore D -80°F to +250°F /de/tds/uv17med
UV18Med
High strength, toughened UV curable system for bonding in medical applications
Dielectric Constant
3.6
Refractive Index
1.524
  • ISO 10993-5 for Cytotoxicity
  • USP Class VI Medical
  • RoHS Compliant
  • Bonding
  • Sealing
1,200-4,800 cps Cures readily in 20-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm, with an energy output as low as 20-40 milliwatts per cm² 50-60 Shore D -60°F to 250°F /de/tds/uv18med
UV18Med-2 UV Curable Adhesive
UV18Med-2
High strength, toughened UV curable system for medical grade applications
Dielectric Constant
3.6 at 75°F, 60Hz
Volume Resistivity
>10¹⁴ ohm-cm
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
1,200-4,800 cps 20-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm, with an energy output as low as 20-40 milliwatts per cm² 50-60 Shore D -60°F to +250°F /de/tds/uv18med-2
 UV19 One Part UV Curable Compound
UV19
Ultra low viscosity, very flexible, UV curing system for bonding, sealing, coating, and encapsulation
Dielectric Constant
3.9
Volume Resistivity
>10¹⁴ ohm-cm
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gap Filling
80-300 cps Cures readily in 10-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts/cm2 40-50 Shore A -80°F to +250°F /de/tds/uv19