Lab Report

Die Shear Strength of Adhesives

Die shear testing is vital to assess the reliability of the adhesive for surface mount and die attach applications. At Master Bond, our adhesives are analyzed by an independent lab for die shear strength. Testing is based on Mil-Std-883 Method 2019. The main objective of die shear testing is to evaluate the adhesive strength between a semiconductor die and the substrate of the package. In this test the force is applied in a perpendicular direction to the die edge, and parallel to the die attach or substrate plane.

Illustration of die shear testing process

The compounds we used for testing are one component electrically conductive as well as non-conductive epoxy systems that have been designed for die attach applications and require heat for curing: Supreme 3HTND-2DA, EP3HTS-TC, EP3HTSDA-2, EP17HTDA-1, and EP17HTDA-2. Using a die size of roughly 2 x 2 mm (80 x 80 mil), the adhesives were applied and cured in accordance with their specifications. Results of the die shear test are indicated in the chart below.

Die Shear Strength Testing Results

Die shear strength test results of select Master Bond adhesives

Disclaimer: The findings in this article are not meant to be used for specification purposes.

Adhesives Featuring High Die Shear Strength

תמונה
Supreme 3HTND-2DA One Part Epoxy
One component, fast curing die attach adhesive. Excellent die shear strength. Serviceable from -100°F to +400°F. Low ionics. Superior thermal conductivity and electrical insulation properties. Dispenses smoothly without tailing or bleed out. Cures in 5-10 minutes at 150°C. NASA low outgassing approved. Available in syringes. Well suited for automatic dispensing. Performed well in 85°C/85% RH testing.
תמונה
One Part, Silver Filled Epoxy EP3HTS-TC
Silver filled electrically conductive, for die attach and general bonding. Low volume resistivity and high temperature resistance. Superior bond strength. Thermally conductive. Thixotropic paste, consistency. Available in syringes that are compatible with various types of automatic dispensers or manual dispensing. Serviceable from -80°F to +400°F.
תמונה
EP3HTSDA-2 One Part Die Attach Epoxy
Silver filled electrically conductive epoxy has a rapid cure speed. Low volume resistivity and high temperature resistance. Superior bond strength. Thermally conductive with incredibly low thermal resistance. Smooth paste, consistency. Available in syringes that are compatible with various types of automatic dispensers or manual dispensing. Serviceable from -80°F to +450°F.
תמונה
EP17HTDA-1 One Part Epoxy
Single component heat curable epoxy adhesive/sealant. Non-drip system. Resists up to 525°F. Meets NASA low outgassing specifications. Meets MIL-STD-883J Section 3.5.2 for thermal stability. High lap shear, tensile and compressive strength. Tg of 230-240°C after post cure.
תמונה
One Part Die Attach Epoxy EP17HTDA-2
One component, heat cured epoxy for bonding and sealing, as well as die attach applications. Flowable, high viscosity system, cures in 4-5 hours at 300°F or 3-4 hours at 350°F. Post cure to optimize properties. High glass transition temperature. NASA low outgassing approved.