Is there a fast curing adhesive that can bond electronic components?

This application highlights fast curing adhesive options for bonding electronic components, including small quartz elements requiring rapid setup and optical clarity. It also reviews key selection factors such as UV or LED accessibility, service temperature, cure speed, optical performance and NASA low outgassing requirements.

Bild
EP30-4 Master Bond Epoxy

The Application

A customer is working on a bonding application involving small quartz elements wherein a fast set up and cure is critical. The other parameter is that the cured adhesive needs to be optically clear.

Finding the Answers

  • What are the configurations of the parts? What are the bonding areas?
  • Would the bonding areas have 100% accessibility to UV (~ 365 nm) or LED (~ 405 nm) light for curing?
  • What are the operating temperatures?
  • Would the adhesive be in the optical path? If so, would there be specific transmission and refractive index needs that have to be met?
  • What are the requirements for the pot life and the cure time?

The Solution

We recommended EP30-4, UV24TKLO and LED401LV.

Based on the answers to the above questions and making certain assumptions, we recommended a few options to consider. They were: EP30-4, UV24TKLO and LED401LV.

EP30-4 is an optically clear, low viscosity, two component room temperature curing epoxy system. It sets up and cures quickly at room temperature.

UV24TKLO and LED401LV are optically clear, moderate viscosity systems. The assumption made here would be that the application areas are accessible to UV (~ 365 nm) and LED (~ 405 nm) light respectively. Also, UV24TKLO meets NASA low outgassing standards.

Additional options:

In certain applications where the optical clarity of the product is not critical, some other products which can be used are two part epoxy systems EP65HT-1 and EP51M; one component EP17HT-3 and one part silicone system MasterSil 711.

Summary of Products

ProductViscosityNASA Low Outgassing ApprovedOptically ClearCure MechanismsTypical Set Up Times
EP65HT-1ModerateYesNoRoom tempMinutes
EP30-4LowNoYesRoom tempMinutes
UV24TKLOModerateYesYesUV light (~365 nm)Seconds
LED401LVModerateNoYesLED light (~405 nm)Seconds
MasterSil 711ModerateNoNoRoom temp (moisture cure)Minutes
EP51MModerateNoNoRoom tempMinutes
EP17HT-3ModerateNoNoHeat cureSeconds
 

Meet Our Tech Expert: Michael Wollman

imageMichael Wollman analyzes application oriented issues and provides solutions in a variety of industries. He has over 30 years experience managing various production facilities, and has a vast understanding of the proper use of adhesives in manufacturing.