USP Class VI approved one and two component adhesives, sealants and coatings are formulated for the assembly of medical devices. These specialty compounds are designed to adhere to dissimilar substrates, resist exposure to sterilization and for easy application.

תמונה
Biocompatible Adhesives, Sealants and Coatings

Key Advantages of Master Bond's Biocompatible Compounds

Medical grade adhesives, sealants, coatings and potting/encapsulation compounds need to be non-toxic and show compatibility with blood and body fluids. Additionally, they must be biologically inert. There are two standard tests used to determine their suitability: U.S. Pharmacopeia (USP) Class VI and/or ISO 10993. Master Bond offers biocompatible compounds, which meet one or both specifications.

General Comparison of Different Chemistries for Medical Device Adhesives

Overview: Epoxies and Silicones

 EpoxiesSilicones
 1-part2-part1-part2-part
ApplicationsBonding, coating, sealing
and potting
Bonding, coating, sealing
and potting
Bonding, coating, and sealingBonding, coating, sealing
and potting
Typical Service 
Temperature Range
4K to 400°F4K to 400°F-75°F to 400°F-65°F to 400°F
Curing
Requirements
Fast cures at elevated temperaturesRoom/heat curing systemsRoom temperature (moisture) curingRoom/heat (addition) curing systems
Key PropertiesStructural, with good temperature resistance and easy processingExcellent chemical resistance, with very good physical strength profileHigh degree of flexibility with no mixing neededExcellent flexibility, and cures in thick sections with low stress imparted

Overview: Other Chemistries

 UV/LED Curing SystemsEpoxy-Polyurethane BlendsCyanoacrylates
ApplicationsBonding, coating, sealing and encapsulationBonding, coating, sealing and pottingBonding, coating, and sealing
Typical Service Temperature Range-60°F to 400°F4K to 250°F-60°F to 250°F
Curing RequirementsLight curing systems (-365 nm to 405 nm) Dual curing with heatRoom/heat curing systemsRoom temperature curing systems
Key PropertiesQuick cure times, along with good optical as well as physical strength characteristicsGood degree of toughness, combining flexibility with good overall physical strength propertiesGood bond strength capability with quick cures for smaller components

Bond Strength

 EpoxiesSiliconesUV/LED Curing SystemsEpoxy-Polyurethane BlendsCyanoacrylates
MetalsExcellentGoodGoodGoodExcellent
PlasticsExcellentFairVery GoodFairVery Good
GlassVery GoodGoodVery GoodGoodVery Good
RubbersVery GoodFairFairGoodGood

Sterilization Resistance

 EpoxiesSiliconesUV/LED Curing SystemsEpoxy-Polyurethane BlendsCyanoacrylates
Repeated AutoclavingExcellentPoorVery GoodPoorPoor
Repeated Chemical Sterilization (Sterrad®)ExcellentPoorVery GoodPoorPoor
Gamma, E-beam, EtO etc.ExcellentExcellentExcellentVery GoodGood

All systems can be applied manually, semi-automatically and automatically.

Sterrad® is a registered trademark of Johnson & Johnson.

Find out more about our full product line of USP Class VI approved adhesive systems.

Find out more about our products meeting ISO 10993-5 cytotoxicity requirement.

Most Popular USP Class VI Approved Products