Fast curing adhesives can cure in minutes, or even seconds, which can improve assembly time and costs. Fast cure adhesives are available as one and two part formulations and come in a range of different chemistries. One-part formulations that cure with the application of heat or UV/LED light have a virtually unlimited open time at room temperature. Two-part formulations cure upon the reaction of their chemical components at ambient temperatures. Gel time for the fastest versions can be minutes, allowing them to be handled or removed from fixtures. To reach their fully cured state can take hours longer. It is important to note that engineers should question if a fast cure is absolutely necessary when selecting an adhesive--there could be trade-offs in the physical properties that would be less suitable for certain bonding, sealing and potting applications.

תמונה
Fast Curing Adhesive Systems for Industrial Applications

Typical Times And Mechanisms For Fast Curing Systems

Systems/PropertiesGel Times @ 75°FCure TimesCure Mechanism
2-component room temperature curable epoxy3-10 minutes12-24 hours at 75°FCross linking at room temperature
1-component heat curable epoxyWill not gel at room temperatures3-10 minutes at 250-350°FHeat activated
1-component cyanoacrylate30-60 seconds12-24 hours at 75°FMoisture/humidity
1-component silicone3-10 minutes12-24 hours at 75°FMoisture/humidity
UV curableWill not gel without UV exposure20-40 seconds with UV light365 nm with minimum 20-40 mW/cm2
UV + heat dual cureWill not gel without UV/heat exposure20-40 seconds with UV + 40-60 minutes with heat365 nm with minimum 20-40 mW/cm2 + heat 180-250°F
LED curableWill not gel without LED exposure20-40 seconds with LED light405 nm with minimum 1-4 W/cm2

Applying a Fast Cure Epoxy

EP65HT-1 is a two part, room temperature curing adhesive that can be applied with a gun applicator. You can see how quickly it sets up in this video.

Performance Properties for Fast Cure Compounds

Master Bond fast curing adhesives are custom formulated to feature outstanding performance properties including chemical resistance, thermal conductivity, high temperature resistance, high strength, low outgassing and more, which can be altered to meet specific requirements.