Tech Tip

Why Use Fungus Resistant Adhesives?

On the most basic level fungal build up on epoxy resin systems weaken the core performance properties of the adhesive itself resulting in adhesive failure. The fungus work to break down the resin into smaller particles as a nutritional source to obtain carbon. Among other things, this degradation causes the adhesive, sealant or encapsulant to lose its ability to protect against chemical and moisture exposure. Below is an outline of the harmful effects of fungus on epoxies:

  • Material Deterioration
    The physical properties of the adhesive are compromised due to the molecular degradation caused by the fungus.
  • Electrical Failures
    At times the fungal growth can create an electrical bridge over insulating materials producing electrical failures.
  • Restricted Movement of Small Parts
    The fungus can fuse together small mechanical parts restricting their movement.
  • Moisture to Non-Wetting Surfaces
    Fungal communities introduce moisture into their living environments which can cause further damage to bonded parts.

How do fungus resistant adhesives work?

Adhesives, sealants, coatings and potting compounds resist fungus

Safeguarding aerospace/military equipment and electronic devices from the harmful effects of these organisms is of prime importance in order to ensure optimal adhesive performance. Fungus resistant adhesives, sealants and encapsulants maintain their physical, mechanical, electrical and optical properties even upon exposure to moisture or warm temperatures. They are engineered to be non-nutrient so that they avoid any degradation including defending against marring of optical components, thwarting the blockage of moving parts, impeding moisture permeation in electronic parts even – upon conditions that are conducive to fungal growth.

How do you test an adhesive’s fungus resistance?

One of the most robust ways of testing adhesives for fungus resistance is with the MIL-STD-810G with Change 1, Method 508.7 standard. This stringent military standard was developed by the U.S. Department of Defense. It is used to determine the extent to which a product will support fungal growth, how that growth can affect the performance of the material, and what specific species have grown. The epoxy samples are inoculated with a spore suspension consisting of the following organisms:

  • Aspergillus flavus
  • Aspergillus versicolor
  • Penicillium funiculosum
  • Chaetomium globosum
  • Aspergillus brasiliensis (formerly known as A.niger)

How is the MIL-STD-810G standard test performed?

MIL-STD-810G with Change 1, Method 508.7 was employed on many Master Bond products to determine their fungus resistance. Products were rated for amount of growth with 0 being devoid of microbial growth and 4 representing massive growth.

Fungus Rating Guideline
Growth AmountRatingObservation
None0Substrate is devoid of microbial growth
Trace1Substrate is devoid of microbial growth.
Light2Intermittent infestations or loosely spread microbial colonies on substrate surface.
Medium3Substantial amount of microbial growth. Substrate may exhibit visible structural change.
Heavy4Massive microbial growth.

Specimens were preconditioned at 30°C and 90% minimum relative humidity within the test chamber. They were then sprayed with prepared spore suspension. The objective was to assess the select adhesive system to ascertain if it would support fungus growth, whether it can function after exposure and identify the species (if growth occurs). Samples were tested for 28 days and exhibited no signs of fungal growth. Specified temperature for test and moisture level was most conducive for spore germination and growth. Sample specimens were compared with a control sample. Below are a handful of the tested epoxies including their test results:

Test Results of Master Bond Fungus Resistant Systems
Part NumberProduct InformationVisual Results After 28 Days
MasterSil 151AOFlexible silicone casting, potting and sealing system with thermal conductivity of 0.35-.0.54 W/(m•K)0 – None
EP36ANB-stage epoxy potting & bonding compound with outstanding toughness and resistance up to 500°F0 – None
EP39MAOHTLow viscosity epoxy with superior dielectric properties resists thermal cycling and mechanical shock0 – None
EP3RR-80One part epoxy cures at 80°C or higher features low exotherm upon cure0 – None
EP30LTE-LOTwo part epoxy with extra low coefficient of thermal expansion and unmatched dimensional stability0 – None
EP37-3FLFAOFlexible, low viscosity, thermally conductive epoxy meets NASA low outgassing specifications0 – None
Control SpecimenConsists of sterile potato dextrose agar and unbleached, plain weave, 100% cotton cloth strips4 - Heavy growth (60% to complete coverage)

Learn more about our systems meeting MIL-STD-810G specifications

Master Bond Fungus Resistant Systems

תמונה
MasterSil 151AO Two Part Silicone System
Thermally conductive silicone casting, potting and sealing system. Thermal conductivity of 0.35-.0.54 W/(m•K). Electrically isolating. Low viscosity system bonds well to a wide variety of substrates. Remarkable flexibility. Temperature resistant from -65°F to +400°F. White color.
תמונה
EP36AN One Component, B-stage Epoxy
Thermally conductive/electrically insulative B-stage epoxy potting/bonding compound. Outstanding toughness and flexibility. Resists up to 500°F. Ability to withstand thermal cycling and impact/vibration. Shore D hardness 80. Volume resistivity 1014 ohm-cm.
תמונה
EP39MAOHT Two Part Epoxy System
Thermally conductive, low viscosity potting/encapsulation compound. Superior dielectric properties. Versatile cure schedules. Convenient one to one mix ratio weight or volume. Minimal shrinkage and stress development. Resists thermal cycling and mechanical shocks. Service temperature range -100°F to +400°F.
תמונה
EP3RR-80: One Part Epoxy System
Moderate viscosity with excellent flow properties. One part system featuring cures at 80°C or higher. Superior thermal conductor. Excellent electrical insulator. Low exotherm while curing. Outstanding mechanical strength properties. Withstands 1,000 hours 85°C/85% RH. Passes NASA low outgassing tests. Serviceable from -100°F to +350°F.
תמונה
EP30LTE-LO Two Part Epoxy Compound
Two component epoxy system. Extra low thermal expansion coefficient and unmatched dimensional stability. Bonding, sealing, casting compound. Passes NASA low outgassing specifications. Room temperature curing. Low shrinkage. Serviceable from 4k to +250°F. Successfully tested for 1,000 hours 85°C/85% RH.
תמונה
EP37-3FLFAO Two Part Epoxy
Flexible, low viscosity, thermally conductive epoxy. Meets NASA low outgassing specifications. Superb electrical insulator. Good physical strength. Chemical resistant. Long working life. Withstands 1,000 hours 85°C/85% RH. Guards against mechanical shock and vibration. Excellent flowability. Ideal for potting and casting.