EP126
Two part epoxy for bonding and sealing featuring very high temperature resistance
Key Features
- Excellent glass transition temperature
- Noteworthy bonding strength
- Outstanding chemical resistance
- Top notch machineablilty
Typical Properties
Viscosity
250,000-500,000 cps
Cure Schedule
3-4 hours at 300°F or 2-3 hours at 350°F
Service Temperature Range
-80°F to +600°F
Dissipation Factor
0.091 @ 75F; 0.034 @ 500F
Glass Transition Temperature (Tg)
160 to 180°C
Image
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
Meets EU Directive 2015/863
Video
EP126: How Do You Mix a Two Part Epoxy When Part B is a Powder?
Watch this demonstration to learn the step by step process of mixing a two part epoxy system, where Part A is a liquid and Part B is a powder. Epoxy system EP126 was used in this video.