EP3HTMed
One part, heat curing, biocompatible epoxy compound
Key Features
- One component, no mix system
- USP Class VI certified
- Passes ISO 10993-5 for cytotoxicity
- Resists repeated sterilization
Typical Properties
Viscosity
100,000-200,000 cps
Cure Schedule
250°F for 20-30 minutes, 300°F for 5-10 minutes, followed by 1 to 3 hours at +250 to +300°F
Hardness
80-90 Shore D
Service Temperature Range
-60°F to +400°F
Tensile Lap Shear Strength
1,600-1,800 psi
Volume Resistivity
>10¹⁴ ohm-cm
Image
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Certifications
ISO 10993-5 for Cytotoxicity
Meets EU Directive 2015/863
USP Class VI Medical
Case Study
EP3HTMed: Relative Biological Effectiveness of Alpha Radiation in Cultured Porcine Aortic Cells
Master Bond EP3HTMed medical grade epoxy was used in a patent in the field of drug delivery and pulmonary therapy, specifically, the aerosolization of liquid medicament into fine liquid droplets for inhalation.
Case Study
EP3HTMed: Utilized in Drug Delivery and Pulmonary Therapy
Master Bond EP3HTMed1 was used in a patent in the field of drug delivery and pulmonary therapy, specifically, the aerosolization of liquid medicament into fine liquid droplets for inhalation.