Toughened, Optically Clear Epoxy EP38CL
Shining a light on incredible toughness, Master Bond EP38CL is a two component epoxy that withstands rigorous thermal cycling and mechanical shock. This durable system also boasts superior optical clarity and a high physical strength profile.
Video Transcript
Master Bond EP38CL sheds light on the importance of toughness and other high performance properties. This two part epoxy is ideal for bonding, sealing, coating, small encapsulations.
EP38CL produces tough, hard bonds and features excellent thermal cycling and impact resistance.
It's easy to see that EP38CL is optically clear and has a glossy appearance.
Its impressive strength profile includes:
- Tensile lap shear strength of 2,500 psi
- Tensile strength of 7,500 psi
- Compressive strength of 8,000 psi
This low viscosity epoxy features:
- 100 to 60 mix ratio by weight
- Long open time of 40-50 minutes
- Room temperature curing
It is easy to apply by brushing or rolling and offers:
- Adhesion to a variety of substrates
- Low shrinkage upon cure
- Shore D hardness >75
- Electrical insulation
EP38CL is the enlightened selection for a wide range of industries, such as:
- Optical
- Electro-optical
- OEM
- Aerospace
For more information contact a technical specialist.