EP41S-6
Two component epoxy system that meets UL 1203 for Explosion-Proof and Dust-Ignition-Proof Electrical Equipment for Use in Hazardous (Classified) Locations
Key Features
- Convenient handling
- Good flow properties
- Black color
- High temperature resistant
Typical Properties
Viscosity
30,000-60,000 cps
Cure Schedule
24 hours at room temperature followed by 10 hours at 125°C
Hardness
85-95 Shore D
Service Temperature Range
-80°F to +500°F
Dielectric Strength
440 volts/mil
Glass Transition Temperature (Tg)
145-150°C
Image
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
Meets EU Directive 2015/863
UL 1203 for Explosion-Proof & Dust-Ignition-Proof