EP21LVTK-2
Two component epoxy system for bonding, sealing, coating, and casting
Key Features
- Convenient handling
- Cures at ambient or elevated temperatures
- Good electrical insulation properties
- Outstanding physical strength
Typical Properties
Viscosity
27,000-33,000 cps
Cure Schedule
overnight at 75°F, followed by a post cure at 150-200°F for 2-3 hours
Hardness
>70 Shore D
Service Temperature Range
-60°F to +250°F
Dielectric Strength
440 volts/mil
Tensile Lap Shear Strength
2,800-3,000 psi