EP41SMed
Two part epoxy system for bonding, sealing, coating and potting that meets USP Class VI and ISO 10993-5 for medical applications
Key Features
- Very fast curing; quick handling time
- Highly resistant to chemical sterilants
- Exellent physical strength properties
- Outstanding electrical insulation properties
Typical Properties
Viscosity
Part A: 10,000-15,000 cps, Part B: 3,000 - 5,000 cps
Cure Schedule
24 hours at 75°F, 60-90 minutes at 200°F, optimum cure schedule overnight at 75°F followed by 1-2 hours at 150-200°F
Hardness
>75 Shore D
Service Temperature Range
-60°F to +250°F
Dielectric Constant
3.6
Volume Resistivity
>10¹⁴ ohm-cm
Image
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
ISO 10993-5 for Cytotoxicity
Meets EU Directive 2015/863
USP Class VI Medical
Packaging