Product Selector

Filters
Applications
Product Type
Certifications
Thermal Conductivity
Product Certifications Applications Viscosity Cure Schedule Hardness Temp. Range Link to Content
LED415DC90Med One Part LED and Heat Curing Adhesive
LED415DC90Med
One component, dual curing LED/heat system that allows for rapid LED initiated fixturing followed by full cure by adding heat; meets ISO 10993-5
Dielectric Constant
4.5
Tensile Modulus
450,000-550,000 psi
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
25,000-250,000 cps cures rapidly upon exposure to LED light at 405 nm followed by heat curing at 90-95°C for 30-45 minutes 85-90 Shore D -80°F to +350°F /tds/led415dc90med
MasterSil 151AO Two Part Silicone System
MasterSil 151AO
Two part silicone for high performance casting, potting & encapsulation and sealing
Coefficient of Thermal Expansion
120-150 X 10⁻⁶ in/in/°C
Dielectric Strength
450 volts/mil
  • MIL-STD-810G for Fungus Resistance
  • RoHS Compliant
  • Encapsulation
  • Potting
  • Sealing
  • Coating
  • Gap Filling
  • Bonding
  • Casting
Part A: 17,000-24,000 cps, Part B: 50-150 cps 48-72 hours at 75°F, 2-3 hours at 200°F 75-85 Shore A -65°F to +400°F /tds/mastersil-151ao
MasterSil 151Med Two Part Silicone
MasterSil 151Med
Two component, biocompatible silicone compound for potting and encapsulation
Acoustical Impedance
1.1 MRayl
Refractive Index
1.43
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • USP Class VI Medical
  • Encapsulation
  • Potting
  • Sealing
  • Coating
  • Gap Filling
  • Bonding
  • Casting
Part A: 2,000-4,000 cps, Part B: 50-150 cps 75°F: 24-48 hours; 200°F: 1-2 hours 40-50 Shore A -65°F to +400°F /tds/mastersil-151med
MasterSil 152 Two Part Silicone System
MasterSil 152
Two component, condensation curing silicone for potting, encapsulation and sealing
Dielectric Strength
450 volts/mil
Refractive Index
1.435
  • RoHS Compliant
  • Sealing
  • Encapsulation
  • Potting
  • Gap Filling
Part A: 500-900 cps, Part B: 50-150 cps Curing is at 75°F only, with a full cure in 24-48 hours 25-35 Shore A -65°F to +400°F /tds/mastersil-152
MasterSil 153 Two Part Silicone
MasterSil 153
Two component, addition cured silicone for bonding and sealing applications
Dielectric Strength
450 volts/mil
Elongation
400-500%
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Part A: 150,000-300,000 cps, Part B: 50,000-250,000 cps At 75°F MasterSil 153 will cure in 48-72 hours. Faster cures can be realized at elevated temperatures, e.g. 2-3 hours at 200°F. 20-35 Shore A -65°F to +400°F /tds/mastersil-153
MasterSil 153AO Two Part Silicone System
MasterSil 153AO
Two part thermally conductive, electrically insulating silicone for bonding and sealing
Dielectric Strength
450 volts/mil
Elongation
100-120%
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Part A: 200,000-550,000 cps, Part B: 100,000-500,000 cps Optimum cure is overnight at 75°F followed by 2-4 hours at 135°F to 185°F. 65-75 Shore A -65°F to +400°F /tds/mastersil-153ao
MasterSil 323AO-LO
Two part thermally conductive, electrically insulating silicone for bonding and sealing
Dielectric Constant
3.7
Dielectric Strength
450 volts/mil
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Gap Filling
300,000-400,000 cps 12-24 hours at 75°F, followed by 3-5 hours at 125°F to 175°F 70-75 Shore A -65°F to +400°F /tds/mastersil-323ao-lo
MasterSil 710 One Part Silicone System
MasterSil 710
One component, silicone elastomer adhesive for high performance bonding and sealing
Dielectric Constant
2.5
Elongation
550-650%
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gasketing
paste Tack-free time, 75°F 7-12 minutes 35-45 Shore A -75°F to +400°F /tds/mastersil-710
MasterSil 711 One Part Silicone System
MasterSil 711
Silicone elastomer adhesive for high performance bonding and sealing
Dielectric Strength
500 volts/mil
Elongation
300-400%
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gasketing
60,000-80,000 cps Tack-free time, 75°F, >50% humidity 2-5 minutes 25-35 Shore A -75°F to +400°F /tds/mastersil-711
MasterSil 910Med
One part, acetoxy type silicone system for high performance bonding, sealing & coating for medical devices
Dielectric Constant
2.75
Elongation
500-600%
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • USP Class VI Medical
  • Bonding
  • Sealing
  • Coating
  • Gasketing
paste Tack-free time, 75°F 10-20 minutes 20-30 Shore A -75°F to +400°F /tds/mastersil-910med

Need Expert Guidance?

Our expert engineers offer one-on-one consultations to help you navigate our extensive material library and find the right solution for your application. We ensure confidentiality and quick turnaround (1-2 business days).