EP79 Two Part Epoxy
EP79
Two component, room temperature curing epoxy for bonding, sealing and coating
Tensile Modulus
300,000-350,000 psi
Volume Resistivity
<0.005 ohm-cm
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
flowable overnight at 75°F followed by a post cure of 1-2 hours at 150-200°F 75-85 Shore D 4K to +275°F /tds/ep79
EP79FL Two Part Epoxy System
EP79FL
Two component, room temperature curing epoxy for bonding, sealing and coating
Thermal Conductivity
12-15 BTU•in/(ft²•hr•°F) [1.73-2.16 W/(m•K)]
Volume Resistivity
<0.005 ohm-cm
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
flowable overnight at 75°F followed by a heat cure of 2-3 hours at 200°F >50 Shore D 4K to +275°F /tds/ep79fl
Low viscosity, optically clear, two part epoxy adhesive
EP88FL
Two component, room temperature curing epoxy for bonding, coating, sealing and potting
Elongation
30-50%
Refractive Index
1.51
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Potting
  • Gap Filling
  • Encapsulation
800-1,200 cps overnight at 75°F followed by 1 to 2 hours at 150°F to 200°F 45-55 Shore D 4K to 250°F /tds/ep88fl
EP90FR-H Two Part Epoxy
EP90FR-H
Two component high strength epoxy system complying with FAR standard 14 CFR 25.853(a) for flame retardancy
Dielectric Constant
4.4
Volume Resistivity
>10¹⁴ ohm-cm
  • RoHS Compliant
  • FAR 25.853(a) for Flame Retardancy
  • Bonding
  • Sealing
  • Coating
  • Potting
  • Gap Filling
  • Encapsulation
  • Casting
20,000-50,000 cps overnight at 75°F followed by 2-3 hours at 150-200°F >80 Shore D -60°F to +250°F /tds/ep90fr-h
EP90FR-HFL Two Part Epoxy
EP90FR-HFL
Two component toughened epoxy system complying with FAR standard 14 CFR 25.853(a) for flame retardancy
Elongation
30-40%
Volume Resistivity
>10¹⁴ ohm-cm
  • FAR 25.853(a) for Flame Retardancy
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
  • Sealing
  • Coating
  • Potting
  • Casting
  • Gap Filling
  • Encapsulation
3,000-10,000 cps overnight at 75°F followed by 3-4 hours at 150-200°F 25-45 Shore D -60°F to +250°F /tds/ep90fr-hfl
EP90FR-V Two Part Epoxy System
EP90FR-V
Two component epoxy system meeting FAR standard 14 CFR 25.853(a) for flame retardancy also passes Boeing standard BSS 7238, Revision C for low smoke and BSS 7239, Revision A for toxicity
Dielectric Constant
4.5
Volume Resistivity
>10¹⁴ ohm-cm
  • RoHS Compliant
  • Boeing Standards for Flame Retardancy
  • FAR 25.853(a) for Flame Retardancy
  • Bonding
  • Sealing
  • Coating
  • Potting
  • Casting
  • Encapsulation
  • Gap Filling
20,000-40,000 cps overnight at 75°F followed by 3-4 hours at 150-200°F >75 Shore D -60°F to +250°F /tds/ep90fr-v
EP93AOFR
Two component thermally conductive flame retardant epoxy system that complies with FAR standard 14 CFR 25.853(a) for flame retardancy
Thermal Conductivity
3.5-4.2 BTU•in/(ft²•hr•°F) [0.5-0.6 W/(m•K)]
Volume Resistivity
>10¹⁴ ohm-cm
  • FAR 25.853(a) for Flame Retardancy
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Potting
  • Encapsulation
  • Casting
  • Gap Filling
30,000-150,000 cps overnight at 75°F followed by 3-4 hours at 150-200°F 80-85 Shore D -80°F to +300°F /tds/ep93aofr
EP93FRHT Two Component Epoxy
EP93FRHT
Two component epoxy system meets the Airbus standards noted below from ABD0031, Issue F, June 8, 2005 for flame retardancy
Dielectric Constant
4.5
Volume Resistivity
>10¹⁴ ohm-cm
  • Airbus Standards for Flame Retardancy
  • RoHS Compliant
  • Bonding
  • Sealing
  • Encapsulation
  • Potting
  • Coating
  • Casting
  • Gap Filling
6,000-9,000 cps overnight at 75°F followed by 3-5 hours at 150-200°F 80-90 Shore D -80°F to +400°F /tds/ep93frht
LED401 One Part LED Curing System
LED401
One component LED curable system for high performance bonding, sealing, coating and encapsulation
Coefficient of Thermal Expansion
60-65 X 10⁻⁶ in/in/°C
Dielectric Constant
4.2
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
100,000-150,000 cps Cure with LED at 405 nm at ~ 1-4 watts/cm² intensity for 15-30 seconds or longer in thicker sections. 65-75 Shore D -60°F to +250°F /tds/led401
LED401 White One Part LED Curing System
LED401 White
One component LED curable system for high performance bonding, sealing, coating and encapsulation
Coefficient of Thermal Expansion
60-65 X 10⁻⁶ in/in/°C
Volume Resistivity
>10¹⁴ ohm-cm
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
100,000-200,000 cps Cure with LED at 405 nm at ~ 1-4 watts/cm² intensity for 15-30 seconds or longer in thicker sections. 65-75 Shore D -60°F to +250°F /tds/led401-white