Product Certifications Applications Viscosity Cure Schedule Hardness Temp. Range Link to Content
MasterSil 157 One Component Silicone
MasterSil 157
Two component, addition curing silicone for potting, encapsulation and sealing
Dielectric Strength
450 volts/mil
Refractive Index
1.43
  • RoHS Compliant
  • Bonding
  • Sealing
  • Encapsulation
  • Potting
  • Coating
  • Gap Filling
Part A: 5,500-6,000 cps, Part B: 100-300 cps 12-24 hours at 75°F, followed by 3-5 hours at 150-200°F 35-45 Shore A -175°F to +500°F /tds/mastersil-157
MasterSil 170 Gel: Two part silicone encapsulant
MasterSil 170 Gel
Two component, addition curing silicone gel for sealing, potting and encapsulation
Dielectric Strength
500 volts/mil
Refractive Index
1.42
  • RoHS Compliant
  • Encapsulation
  • Potting
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
1,000 cps 24-48 hours at ambient temperatures, or in 1-2 hours at 150-170°F 65 mm penetration -67°F to +392°F /tds/mastersil-170-gel
MasterSil 323
Two component, addition cured silicone for bonding, sealing, and small encapsulations
Elongation
150-250%
Refractive Index
1.44
  • RoHS Compliant
  • Bonding
  • Sealing
  • Encapsulation
  • Coating
  • Gap Filling
  • Potting
Part A: 15,000-30,000 cps, Part B: 10,000-25,000 cps 48-72 hours at 75°F or 2-4 hours at 135-165°F 35-45 Shore A -65°F to +400°F /tds/mastersil-323
MasterSil 323Med
Two component, medical grade silicone for bonding and sealing
Acoustical Impedance
1.1 MRayl
Elongation
150-250%
  • RoHS Compliant
  • ISO 10993-5 for Cytotoxicity
  • Bonding
  • Sealing
  • Encapsulation
  • Potting
  • Gap Filling
Part A: 15,000-30,000 cps, Part B: 10,000-25,000 cps 75°F: 48-72 hours; 135-165°F: 2-4 hours; Optimal cure: Overnight at 75°F followed by 2-4 hours at 135-165°F 35-45 Shore A -65°F to +400°F /tds/mastersil-323med
MasterSil 323Med Black Two Part Medical Silicone
MasterSil 323Med Black
Two component, medical grade silicone for bonding and sealing
Dielectric Strength
450 volts/mil
Elongation
150-250%
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • Bonding
  • Sealing
  • Encapsulation
  • Coating
  • Gap Filling
Part A: 15,000-30,000 cps, Part B: 10,000-25,000 cps cures at ambient temperatures in 48-72 hours or in 2-4 hours at 135-165°F; optimum cure is overnight at 75°F followed by 2-4 hours at 135-165°F 35-45 Shore A -65°F to +400°F /tds/mastersil-323med-black
Master Bond MasterSil 323S-LO Silicone System
MasterSil 323S-LO
Two part, silver filled, low outgassing silicone for bonding, sealing and coating
Elongation
50-100%
Volume Resistivity
<0.003 ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Part A: paste, Part B: paste 8-12 hours at 130-150°F, 4-6 hours at 160-180°F or 2-3 hours at 190-210°F 35-55 Shore A -80°F to +400°F /tds/mastersil-323s-lo
MasterSil 415 One Part Silicone Elastomer
MasterSil 415
One component silicone elastomer adhesive for high performance bonding and sealing
Dielectric Strength
500 volts/mil
Elongation
350-450%
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste 12-24 hours at 75°F 25-35 Shore A -185°F to +400°F /tds/mastersil-415
MasterSil 705 One Component Silicone
MasterSil 705
One component, silicone elastomer adhesive for high performance bonding and sealing
Dielectric Constant
2.5
Elongation
300-400%
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gasketing
paste Cures at 75°F 25-35 Shore A -75°F to +450°F /tds/mastersil-705
MastersSil 705S One Component Silicone
MasterSil 705S
One component, non-corrosive silicone for bonding and sealing
Elongation
50%
Volume Resistivity
<0.01 ohm-cm
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gasketing
paste Tack-free time, 75°F for 15-20 minutes 70 Shore A -60°F to +400°F /tds/mastersil-705s
MasterSil 705TC One Part Silicone
MasterSil 705TC
One component, non-corrosive silicone for bonding, sealing & coating
Dielectric Constant
4.2
Elongation
70%
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gasketing
paste Tack-free time, 75°F 7 minutes 70-80 Shore A -60°F to +400°F /tds/mastersil-705tc