Supreme 11AOHT-LO Two Part Epoxy System
Supreme 11AOHT-LO
Toughened, high strength, two component epoxy for bonding and sealing
Coefficient of Thermal Expansion
35-40 X 10⁻⁶ in/in/°C
Tensile Lap Shear Strength
3,200-3,400 psi
  • 1,000 Hours at 85°C/85% RH
  • RoHS Compliant
  • NASA Low Outgassing
  • Bonding
  • Sealing
  • Coating
Part A: 200,000-300,000 cps, Part B: paste overnight at 75°F followed by a few hours at 150-200°F 80-90 Shore D -112°F to +400°F /tds/supreme-11aoht-lo
Supreme 11AOHTLP Two Part Epoxy
Supreme 11AOHTLP
Two component, thermally conductive, electrically insulative epoxy for bonding, sealing and coating
Dielectric Constant
4.6
Tensile Modulus
400,000-450,000 psi
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste overnight at 75°F followed by 3-4 hours at 150-200°F 85-90 Shore D -112°F to +400°F /tds/supreme-11aohtlp
Master Bond Supreme 11AOHTMed Epoxy System
Supreme 11AOHTMed
Toughened, high strength, two component epoxy for bonding and sealing
Dielectric Constant
4.6
T-peel Strength
15-20 pli
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Part A: 200,000-300,000 cps, Part B: paste 75°F: 24-36 hours; 200°F: 1-2 hours 80-90 Shore D -112°F to +400°F /tds/supreme-11aohtmed
Supreme 11HT Two Part Epoxy
Supreme 11HT
Toughened, two component epoxy for bonding, sealing and coating
Coefficient of Thermal Expansion
45-50 X 10⁻⁶ in/in/°C
Tensile Lap Shear Strength
3,200-3,400 psi
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Part A: 90,000-120,000 cps, Part B: 60,000-110,000 cps overnight at 75°F, followed by 1 hour at 150-200°F 75-85 Shore D -112°F to +400°F /tds/supreme-11ht
Two Part Epoxy Supreme 121AO
Supreme 121AO
Two part toughened epoxy for bonding, sealing and encapsulation features good thermal conductivity
Glass Transition Temperature (Tg)
200-210°C
Thermal Conductivity
4-5 BTU•in/(ft²•hr•°F)
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Encapsulation
  • Potting
  • Coating
  • Gap Filling
10,000-25,000 cps 1-2 hours at 200-210°F followed by 3-4 hours at 250°F and then 4-6 hours at 300°F. Additional post curing at 350°F for 2-4 hours will further enhance product properties. 85-95 Shore D -80°F to +550°F /tds/supreme-121ao
Two Part Epoxy Supreme 121AOMed
Supreme 121AOMed
Two part toughened epoxy for bonding, sealing and potting featuring good thermal conductivity and high temperature resistance; requires oven curing
Glass Transition Temperature (Tg)
200-210°C
Thermal Conductivity
4-5 BTU•in/(ft²•hr•°F) [0.58-0.72 W/(m•K)]
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • Bonding
  • Sealing
  • Encapsulation
  • Potting
  • Coating
  • Gap Filling
10,000-25,000 cps 1-2 hours at 200-210°F followed by 3-4 hours at 250°F and then 4-6 hours at 300°F. Additional post curing at 350°F for 2-4 hours will further enhance product properties. 85-95 Shore D -80°F to +550°F /tds/supreme-121aomed
Supreme 121AOND Two Part Epoxy
Supreme 121AOND
Two part toughened epoxy for bonding, sealing and encapsulation features good thermal conductivity
Glass Transition Temperature (Tg)
200-210°C
Thermal Conductivity
4-5 BTU•in/(ft²•hr•°F)
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste 1-2 hours at 200-210°F followed by 3-4 hours at 250°F and then 4-6 hours at 300°F. Additional post curing at 350°F for 2-4 hours will enhance properties. 85-95 Shore D -80°F to +550°F /tds/supreme-121aond
Supreme 12AOHT-LO Epoxy System
Supreme 12AOHT-LO
One part, thermally conductive, electrically insulating, high performance epoxy for bonding and sealing; meets NASA low outgassing specifications
Glass Transition Temperature (Tg)
135-140°C
Tensile Lap Shear Strength
3,400-3,600 psi
  • 1,000 Hours at 85°C/85% RH
  • MIL-STD-883J for Thermal Stability
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste 125°C (257°F) in 60-70 minutes and 150°C (302°F) in 40-50 minutes 80-90 Shore D 4K to +500°F /tds/supreme-12aoht-lo
One Part Epoxy System
Supreme 17HT
One component toughened epoxy system for bonding and sealing
Glass Transition Temperature (Tg)
208-210°C
Tensile Lap Shear Strength
1,900-2,100 psi
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
100,000-150,000 cps 300°F for 4-6 hours, plus 8-12 hours at 350°F. 80-90 Shore D -100°F to +550°F /tds/supreme-17ht
Supreme 17HTMed One Part Epoxy
Supreme 17HTMed
One component, medical grade toughened epoxy system for bonding and sealing
Glass Transition Temperature (Tg)
208-210°C
Tensile Lap Shear Strength
1,900-2,100 psi
  • RoHS Compliant
  • ISO 10993-5 for Cytotoxicity
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
100,000-150,000 cps 4-6 hours at 300°F or 2-4 hours at 350°F 80-90 Shore D -100°F to +550°F /tds/supreme-17htmed