UV21 One Part UV Curable System
UV21
UV system for high performance bonding, sealing, coating, encapsulation and formed-in-place gaskets
Elongation
>250%
Refractive Index
1.49
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gasketing
30,000-80,000 cps cures readily in 10-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts/cm2 40-60 Shore A -65°F to +250°F /tds/uv21
UV22 One Part UV Curable Epoxy
UV22
One component, optically clear, nanosilica filled UV curable epoxy system; meets NASA low outgassing specification
Coefficient of Thermal Expansion
30-35 ppm/°C
Refractive Index
1.52
  • 1,000 Hours at 85°C/85% RH
  • RoHS Compliant
  • ASTM D4060-14 for Abrasion Resistance
  • NASA Low Outgassing
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
2,000-6,000 cps UV light 320-365 nm for 15-45 seconds 75-85 Shore D -80°F to +350°F /tds/uv22
UV22DC80-10F One Part UV System
UV22DC80-10F
One component, nanosilica filled, dual cure system with UV and heat curing mechanisms
Glass Transition Temperature (Tg)
130-135°C
Refractive Index
1.52
  • RoHS Compliant
  • NASA Low Outgassing
  • Bonding
  • Coating
  • Encapsulation
  • Sealing
5,000-15,000 cps Cures at 80°C in shadowed out areas; typically the UV portion occurs in 10-30 seconds at 365 nm with 10-40 milliwatts/cm2 of output; areas not cured because of shadowing effects can be readily cured at 80°C for 30-60 minutes; post curing at 125-150°C for 15-30 minutes will increase the To significantly. 75-85 Shore D -100°F to +350°F /tds/uv22dc80-10f
UV Dual Curing System UV22DC80-1Med
UV22DC80-1Med
One component, nanosilica filled, dual cure system with UV and heat curing mechanisms passes ISO 10993-5 for cytotoxicity and USP Class VI
Dielectric Constant
3.85
Glass Transition Temperature (Tg)
120-130°C
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • USP Class VI Medical
  • Bonding
  • Coating
  • Sealing
  • Gap Filling
  • Underfill
  • Encapsulation
  • Potting
500-3,500 cps UV light 320-365 nm for 20-30 seconds, followed by 80°C for 1 hour 80-90 Shore D -60°F to +350°F /tds/uv22dc80-1med
Nanosilica Filled, UV Dual Cure System
UV22DC80ND
One component, nanosilica filled, dual cure system with UV and heat curing mechanisms
Coefficient of Thermal Expansion
30-35 X 10⁻⁶ in/in/°C
Glass Transition Temperature (Tg)
130-135°C
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Gap Filling
  • Coating
paste 10-30 seconds at 365 nm with 10-40 milliwatts/cm2 of output; areas not cured can be cured at 80°C for 30-60 minutes; post curing at 125-150°C for 15-30 minutes 75-85 Shore D -60°F to +350°F /tds/uv22dc80nd
UV22DC80TK One Part, Dual UV and Heat Curing System
UV22DC80TK
One component, nanosilica filled, dual cure system with UV and heat curing mechanisms
Coefficient of Thermal Expansion
30-35 x 10⁻⁶ in/in/°C
Refractive Index
1.52
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Coating
  • Gap Filling
  • Sealing
  • Encapsulation
40,000-80,000 cps Typically the UV portion occurs in 10-30 seconds at 365 nm with 10-40 milliwatts/cm2 of output. Areas not cured because of shadowing effects can be readily cured at 80°C for 30-60 minutes. Post curing at 125-150°C for 15-30 minutes will increase the Ta significantly. 75-85 Shore D -60°F to +350°F /tds/uv22dc80tk
UV23FLDC-80 UV Curable Adhesive
UV23FLDC-80
One component, dual curing (UV light and heat) that cures with good flexibility
Dielectric Constant
4.7
Elongation
90-100%
  • RoHS Compliant
  • Bonding
100-400 cps 20-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts per cm²; secondary curing in shadowed out areas by heating, typically 60-90 minutes at 80-85°C 45-55 Shore D -80°F to +300°F /tds/uv23fldc-80
One Part, Dual Curing Adhesive UV23FLDC-80TK
UV23FLDC-80TK
One component, UV and heat curable epoxy system with moderate viscosity that cures with good flexibility
Dielectric Constant
4.7
Elongation
90-100% at 75°F
  • RoHS Compliant
  • Encapsulation
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
25,000-50,000 cps initial cure utilizing UV light along with secondary curing in shadowed out areas by heating, typically 60-90 minutes at 80-85°C 45-55 Shore D -80°F to +300°F /tds/uv23fldc-80tk
UV25 UV Curable Adhesive System
UV25
One part, moderate viscosity UV curable system meets NASA low outgassing specifications
Glass Transition Temperature (Tg)
180-185°C
Refractive Index
1.55
  • NASA Low Outgassing
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
7,000-11,000 cps cures readily in 20-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts per cm² 80-90 Shore D -60°F to +500°F /tds/uv25
UV curable adhesive with high thermal stability UV26
UV26
One part, low viscosity UV curable system featuring high temperature resistance for bonding
Glass Transition Temperature (Tg)
160 to 170°C
Refractive Index
1.55
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
250-1,500 cps UV light 320-365 nm for 10-20 seconds 80-90 Shore D -60°F to +500°F /tds/uv26