One component paste consistency epoxy system for bonding, sealing and coating

Key Features

  • Very fast cure
  • High shear strength properties
  • Unlimited working life at room temperature
  • Wide service temperature range of -60°F to +400°F
  • Superb thermal and electrical insulator
  • Withstands 1,000 hours 85°C/85% RH

Product Description

Master Bond EP3HTND-2 combines easy processing with excellent physical and bonding strength properties. It is a one part system requiring no mixing and can be stored at room temperature or in a refrigerator. While it needs oven curing with a minimum temperature of 250°F, it is exceptionally fast curing at that temperature (even faster at higher temperatures). It bonds well to a wide variety of substrates including glass, metals, ceramics and most plastics and has superb physical strength properties. EP3HTND-2 also offers good electrical insulation properties. The service temperature is -60°F to +400°F. It is 100% reactive and does not contain any diluents or solvents. EP3HTND-2 possesses superior chemical resistance to water, oils, fuels and many acids and bases. The color of EP3HTND-2 is brown to tan. This epoxy is widely used in the aerospace, electronics, electrical and OEM industries where superior physical properties, fast curing and high performance are essential.

Product Advantages

  • Single component system; no mixing required
  • Minimum cure temperature of 250°F
  • Easy application; contact pressure only required during heat cure; adhesive spreads evenly and smoothly
  • Fast curing with versatile cure schedules; 5-10 minutes at 300°F, 20-30 minutes at 250°F
  • Good adhesion to many substrates and superior physical properties
  • Excellent bonding strength

Industrial Certifications


1,000 Hours at 85°C/85% RH

Meets EU Directive 2015/863

Packaging


Jar

Syringe

EP3HTND-2 is available is various sizes and units to accommodate customer's needs.