EP64Med

Two component, medical grade epoxy with convienent handling featuring outstanding temperature and chemical resistance

Key Features
  • Long open time at room temperature
  • Convenient elevated temperature cure
  • High glass transition temperature
  • Passes ISO 10993-5

 

Typical Properties
Viscosity
50,000-90,000 cps
Cure Schedule
80-90°C for 4-5 hours, followed by a post cure at 120-130°C for 2-3 hours
Hardness
80-90 Shore D
Service Temperature Range
-60°F to +450°F [-51°C to +232°C]
Glass Transition Temperature (Tg)
210-215°C
Volume Resistivity
>10¹⁴ ohm-cm
Image
Two Part Epoxy System EP64Med
Certifications

Meets EU Directive 2015/863

ISO 10993-5 for Cytotoxicity

Product Description

Master Bond EP64Med is a two component epoxy system with a long working life at ambient temperature. It has a forgiving 100-to-5 mix ratio by weight and, once combined, forms a moderate viscosity mixture that flows well. A 100-gram batch offers a 12–24 hour working life at room temperature. The recommended cure schedule is 80-90°C for 4-5 hours, followed by a post cure at 120-130°C for 2-3 hours. The epoxy contains no solvents or diluents and has low shrinkage upon curing.

The system bonds well to a wide variety of substrates such as metals, plastics, rubbers, ceramics and composites. Upon curing, EP64Med features an exceptionally high glass transition temperature of 210°C which ultimately translates into superb temperature and chemical resistance. The epoxy withstands repeated sterilization including steam and aggressive chemicals. EP64Med is a dependable electrical insulating material. The service temperature range is -60°F to +450°F. The color of Part A is clear and Part B is dark brown. This system is particularly well suited for medical applications that require frequent, aggressive sterilization.

Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.