Master Bond EP42HT-2FG is a food grade adhesive that complies with the rigorous FDA 175.300 and NSF/ANSI 51.4.1 (2009 standard for food equipment) as well as the FDA 175.105 requirements. Moreover, it also meets the USP Class VI requirements for biocompatibility testing and ISO 10993-5 requirements for cytotoxicity testing. Researchers1 used food grade EP42HT-2FG epoxy in developing a novel approach for ensuring precise measurement of pharmaceutical powders for reliable production of pharmaceutical tablets. Read more about the application which successfully demonstrated the non-invasive, continuous, quantitative detection of powder level and mass holdup in a metal feed tube.
To learn more, please download the case study now.
Sources
1 Louge, M. Y., Mandur, J., Blincoe, W., Tantuccio, A., & Meyer, R. F. (2021). Non-invasive, continuous, quantitative detection of powder level and mass holdup in a metal feed tube. In Powder Technology (Vol. 382, pp. 467–477). Elsevier BV. https://doi.org/10.1016/j.powtec.2020.12.068