Supreme 42HT-2ND Black Two Part Epoxy Supreme 42HT-2ND Black

Non-drip epoxy paste, black in color, has outstanding temperature and chemical resistance. Superior toughness and thermal cycling capability. Meets low outgassing specifications. Withstands 1,000 hours 85°C/85% RH. Superb electrical insulator. Service temperature range -80°F to +450°F.

EP101HTX-3 One Part Epoxy System EP101HTX-3

Optically clear one component epoxy has outstanding electrical insulation properties. Viscosity 300-1,000 cps. Service temperature range from -60 to +500°F. Excellent thermal shock resistance.

EP110F6 Two Component Epoxy EP110F6

High performance two component epoxy system for potting, sealing, encapsulating and casting. Medium viscosity liquid with good flowability. Exceptional thermal shock resistance. Superb mechanical and electrical insulation properties. Serviceable from -55°C to +155°C.

EP110F8-1 Two Part Epoxy EP110F8-1

High performance two component epoxy system for potting, sealing, encapsulating and casting. Low viscosity liquid with good flowability. Exceptional thermal shock resistance. Superb mechanical and electrical insulation properties. Serviceable from-80°F to +325°F.

EP110F8-3 Two Part Epoxy EP110F8-3

High performance two component epoxy system for potting, sealing, encapsulating and casting. Low viscosity liquid with good flowability. Exceptional thermal shock resistance. Superb mechanical and electrical insulation properties. Serviceable from -100°F to +300°F.

EP110F8-5 Two Part Epoxy EP110F8-5

High performance two component epoxy system for potting, sealing, encapsulating and casting. Moderate viscosity with good flow. Enhanced dimensional stability and superior thermal cycling resistance. Superb mechanical and electrical insulation properties. Serviceable from -100°F to +300°F.

EP112 Two Part Epoxy EP112

Potting, encapsulation, coating, sealing, impregnation compound. Superior optical clarity and physical strength.Low dielectric constant and low dissipation factor. Stands up to 1,000 hours 85°C/85% RH. Long working life. Serviceable from -60°F to 450°F.

EP112LS Two Part Heat Curing Epoxy EP112LS

Potting, encapsulation, sealing and impregnation compound. Low viscosity two component epoxy system. Heat curable. Long working life at room temperature. Superb optical clarity. Non-yellowing. Serviceable from -60°F to +450°F. High dielectric strength.

EP112M Two Component Epoxy EP112M

Medium viscosity heat curing cycloaliphatic epoxy resin system. Outstanding arc, corona and tracking resistance. Excellent dielectric properties. Resilient. Good endurance in outdoor/indoor environments. High bond strength. Low shrinkage. Serviceable from -60°F to +500°F.

EP113 Two Component Epoxy EP113

Two component nanosilica filled epoxy for potting, coating and sealing. Optically clear. Low shrinkage. Superior electrical insulation properties. Toughened system. Successfully tested for 1,000 hours 85°C/85% RH. Serviceable from -100°F to +450°F.