Product Selector

Filters
Applications
Product Type
Product Type
Certifications
Thermal Conductivity
Product Certifications Applications Viscosity Cure Schedule Hardness Temp. Range Link to Content
EP21LV-LO Two Part Epoxy
EP21LV-LO
Two component, low viscosity NASA low outgassing epoxy compound
Dielectric Constant
2.79
Tensile Lap Shear Strength
2,600-2,800 psi
  • 1,000 Hours at 85°C/85% RH
  • RoHS Compliant
  • NASA Low Outgassing
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gap Filling
  • Potting
  • Casting
10,000-13,000 cps overnight at 75°F followed by 2 hours at 150-200°F 70-80 Shore D -65°F to +250°F /tds/ep21lv-lo
EP21LVFL
Two component, low viscosity epoxy for bonding, sealing, coating, and potting featuring good flexibility
Elongation
120-150%
Volume Resistivity
>10¹⁵ ohm-cm
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gap Filling
10,000-14,000 cps overnight at 75°F followed by 4-6 hours at 125-150°F 40-50 Shore D -100°F to +250°F /tds/ep21lvfl
EP21LVSP6 Two Component Epoxy
EP21LVSP6
Two component epoxy for bonding, sealing, coating and encapsulating
Dielectric Strength
450 volts/mil
Volume Resistivity
>10¹⁴ ohm-cm
  • RoHS Compliant
  • MIL-STD-810G for Fungus Resistance
  • Bonding
  • Sealing
  • Coating
  • Casting
  • Encapsulation
Part A: 1,500-3,000 cps, Part B: 5,000-8,000 cps 75°F: 3-5 days; 200°F: 3-4 hours. 65-75 Shore D -60°F to +250°F /tds/ep21lvsp6
EP21LVTK-2 Two Part Epoxy System
EP21LVTK-2
Two component epoxy system for bonding, sealing, coating, and casting
Dielectric Strength
440 volts/mil
Tensile Lap Shear Strength
2,800-3,000 psi
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Potting
  • Gap Filling
27,000-33,000 cps overnight at 75°F, followed by a post cure at 150-200°F for 2-3 hours >70 Shore D -60°F to +250°F /tds/ep21lvtk-2
EP21ND Two Part Epoxy
EP21ND
Two component epoxy compound for high performance applications
Dielectric Constant
2.92
Tensile Lap Shear Strength
>2,500 psi
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste 48-72 hours at 75°F >70 Shore D -60°F to +250°F /tds/ep21nd
EP21ND-2 Two Part Epoxy
EP21ND-2
Two component epoxy compound for high performance applications
Dielectric Constant
2.92
Tensile Lap Shear Strength
>2,500 psi
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
paste 75°F: 48-72 hours; 200°F: 2-3 hours; Optimum cure schedule: 12-24 hours at 75°F, plus 2 hours at 150-200°F >70 Shore D -60°F to +250°F /tds/ep21nd-2
EP21ND-LO Two Part Non-Drip Epoxy
EP21ND-LO
Two component, non-drip epoxy system for bonding, sealing and coating applications
Dielectric Constant
2.92 at 75°F, 60 Hz
Tensile Lap Shear Strength
>2,500 psi at 75°F
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste 12-24 hours at 75°F, plus another 2 hours at 150-200°F >70 Shore D -60°F to +250°F /tds/ep21nd-lo
EP21ND-LP Two Part Epoxy
EP21ND-LP
Two component epoxy compound for high performance applications featuring convenient handling and a long working life
Dielectric Constant
2.92
Tensile Lap Shear Strength
2,600-2,800 psi
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste 75°F: 3-4 days; 150-200°F: 3-4 hours; Optimum cure schedule: 12-24 hours at 75°F, plus 3 hours at 150-200°F 70-80 Shore D -60°F to +250°F /tds/ep21nd-lp
EP21NDCL Two Part Epoxy System
EP21NDCL
Two component epoxy compound for high performance bonding, sealing and coating
Tensile Lap Shear Strength
2,600-2,800 psi
Volume Resistivity
>10¹⁴ ohm-cm
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste 75°F: 48-72 hours 70-80 Shore D -60°F to +250°F /tds/ep21ndcl
EP21NDFG Two Component Epoxy
EP21NDFG
Two component epoxy compound for high performance applications
Tensile Lap Shear Strength
>2500 psi
Volume Resistivity
>10¹⁴ ohm-cm
  • FDA Food Grade 21 CFR 175.105
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste 48-72 hours at 75°F >70 Shore D -60°F to +250°F /tds/ep21ndfg

Need Expert Guidance?

Our expert engineers offer one-on-one consultations to help you navigate our extensive material library and find the right solution for your application. We ensure confidentiality and quick turnaround (1-2 business days).