EP21TDCS-LO Two Part Adhesive System
EP21TDCS-LO
Durable, high strength two component epoxy for bonding and sealing
Tensile Lap Shear Strength
600-800 psi
Volume Resistivity
0.001 ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste Optimum cure schedule: Overnight at 75°F followed by 2-3 hours at 135-165°F. 40-50 Shore D 4K to +275°F /tds/ep21tdcs-lo
EP21TDCSFL Two Part Conductive Epoxy
EP21TDCSFL
Two component, silver conductive epoxy for high performance bonding, coating and sealing
T-peel Strength
10-15 pli
Volume Resistivity
<0.001 ohm-cm
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Part A: 40,000-60,000 cps, Part B: 50,000-70,000 cps Optimum cure being overnight at ambient temperature followed by a heat cure at 150-200°F for 2-3 hours. 30-40 Shore D 4K to +275°F /tds/ep21tdcsfl
EP21TDCSMed Two Part Medical Grade Epoxy
EP21TDCSMed
Silver conductive, two component epoxy for medical applications
Tensile Lap Shear Strength
800-1,000 psi
Volume Resistivity
less than 0.001 ohm-cm
  • RoHS Compliant
  • USP Class VI Medical
  • ISO 10993-5 for Cytotoxicity
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste overnight at 75°F followed by 2-3 hours at 150-200°F 50-60 Shore D 4K to +250°F /tds/ep21tdcsmed
EP21TP-2NV
Two component, epoxy polysulfide for bonding, sealing, coating and encapsulation
Dielectric Constant
3.7
Elongation
40-80%
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gap Filling
Part A: 4,500-7,500 cps, Part B: 500-3,000 cps 75°F 48-72 hours 40-50 Shore D -80°F to +250°F /tds/ep21tp-2nv
EP21TPFL-1 Two Component Epoxy Polysulfide
EP21TPFL-1
Two component, low viscosity epoxy polysulfide for bonding, sealing, coating and casting
Dielectric Constant
3.9
Elongation
>250%
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Casting
2,000-4,000 cps Cure at 75°F, 3-5 days 30-50 Shore A -60°F to +250°F /tds/ep21tpfl-1
EP21TPFL-1AO Two Part Epoxy Polysuifide System
EP21TPFL-1AO
Flexible two component epoxy polysulfide system for high performance bonding, sealing, coating and potting
Dielectric Constant
4.5
Elongation
150-200%
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
Part A: 15,000-30,000 cps, Part B: 14,000-28,000 cps 75°F, 3-5 days 70-90 Shore A -60°F to +250°F /tds/ep21tpfl-1ao
EP21TPHT Two Part Epoxy
EP21TPHT
Two component, epoxy polysulfide for bonding, sealing, coating and encapsulation
Dielectric Constant
3.9
Elongation
20-40%
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
Part A: 90,000-140,000 cps, Part B: 500 - 2,000 cps 48-72 hours at 75°F; optimum cure overnight at 75°F, followed by 2-3 hours at 150°F 55-65 Shore D -80°F to +350°F /tds/ep21tpht
Two Part Epoxy EP21TPLV-NV
EP21TPLV-NV
Two component, room temperature curing epoxy polysulfide system
Dielectric Constant
4.1
Elongation
40-80%
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gap Filling
Part A: 3,000-4,000 cps, Part B: 500-2,000 cps 75°F: 48-72 hours 40-50 Shore D -80°F to +250°F /tds/ep21tplv-nv
EP21TPND-NV Two Component Epoxy Polysulfide
EP21TPND-NV
Two component, paste-like epoxy polysulfide for bonding, sealing and coating
Dielectric Constant
3.7
Elongation
20-30%
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste 48-72 hours at 75°F 40-50 Shore D -80°F to +250°F /tds/ep21tpnd-nv
EP22 Two Part Epoxy Adhesive System
EP22
Aluminum filled, two component epoxy adhesive for bonding, sealing and coating
Coefficient of Thermal Expansion
35-40 in/in X 10⁻⁶/°C
Dielectric Constant
7.5
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Part A: 70,000-100,000 cps, Part B: 100,000-150,000 cps 75°F: 48-72 hours; 200°F: 2-3 hours >80 Shore D -60°F to +250°F /tds/ep22