EP93FRHT
Two component epoxy system meets the Airbus standards noted below from ABD0031, Issue F, June 8, 2005 for flame retardancy
Key Features
- Twelve second vertical burn per AITM 2.0002B and Section 7.1.2 of ABD0031, Issue F
- Smoke emission per AITM 2.0007B, Issue 3 in the flaming mode and Section 7.3.2 of ABD0031, Issue F
- Toxic gas emission per AITM 3.0005, Issue 2 in the flaming mode and Section 7.4 of ABD0031, Issue F
Typical Properties
Viscosity
6,000-9,000 cps
Cure Schedule
overnight at 75°F followed by 3-5 hours at 150-200°F
Hardness
80-90 Shore D
Service Temperature Range
-80°F to +400°F
Dielectric Constant
4.5
Volume Resistivity
>10¹⁴ ohm-cm
Image
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
Airbus Standards for Flame Retardancy
Meets EU Directive 2015/863
Packaging
Video
Product Spotlight: EP93FRHT
Specifically designed for avionic/aviation applications, Master Bond EP93FRHT readily passes the stringent Airbus specifications for vertical burn test, smoke emission and toxic gas emission as listed under ABD 0031, Issue F.
This video explain …