EP62-1HTND

Two component epoxy system featuring superior temperature and unsurpassed chemical resistance, especially to acids

Key Features
  • Paste consistency
  • Long open time at room temperature
  • Cures at moderately elevated temperatures
  • Superb physical strength profile
Typical Properties
Viscosity
Part A: paste, Part B:100-1,000 cps
Cure Schedule
60-70 minutes at 176-212°F [80-100°C] or 20-30 minutes at 257°F [125°C]. To obtain optimum properties, post curing at 212-302°F [100-150°C] for 3-5 hours is recommended
Hardness
80-90 Shore D
Service Temperature Range
-60°F to +450°F
Glass Transition Temperature (Tg)
145-155°C
Tensile Modulus
500,000-550,000 psi
Image
Two Part Epoxy EP62-1HTND
Applications
Certifications

Meets EU Directive 2015/863

Packaging
Product Description

Master Bond EP62-1HTND is a two component epoxy system with a long working life at ambient temperature. The mix ratio is a forgiving 100 to 5 by weight. Upon mixing, it has a non-drip paste consistency with no flow. The working life of 100 grams is 12-24 hours at room temperature.

There are two cure schedule options, both require the addition of heat. These include 60-70 minutes at 176-212°F [80-100°C] or 20-30 minutes at 257°F [125°C]. To obtain optimum properties, post curing at 212-302°F [100-150°C] for 3-5 hours is recommended. When cured using the optimum schedule, EP62-1HTND displays robust temperature resistance with a glass transition temperature ranging from 145-155°C. It offers excellent resistance to a wide range of aggressive chemicals—particularly acids, as well as many bases and solvents—even at elevated temperatures. EP62-1HTND is a dependable electrically insulating material. The service temperature range is -60°F to +450°F. The color of Part A is translucent and Part B is dark brown. It is well suited for many rigorous applications in aerospace, electronic and specialty OEM, among other industries, especially where high temperature resistance and the ability to withstand hostile chemicals is needed.

Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.