Product Selector

Filters
Applications
Product Type
Product Type
Certifications
Thermal Conductivity
Product Certifications Applications Viscosity Cure Schedule Hardness Temp. Range Link to Content
EP4G-80Med
One component, medical grade, graphite filled epoxy with a curing temperature of 80°C
Glass Transition Temperature (Tg)
130-140°C
Volume Resistivity
50-100 ohm-cm
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
4,000-10,000 cps 60-90 minutes at 80°C 75-85 Shore D -58°F to +347°F /tds/ep4g-80med
One Part Epoxy System EP4NS-80
EP4NS-80
One component, optically clear nanosilica filled epoxy for bonding and sealing with curing temperature of 80°C to 85°C. Meets NASA low outgassing.
Refractive Index
1.52
Tensile Modulus
>1,000,000 psi
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Impregnation
  • Underfill
250-750 cps 2-4 hours at 80°C followed by 1-2 hours at 110-125°C 85-95 Shore D -80°F to +450°F /tds/ep4ns-80
One Part, Silver Filled Epoxy
EP4S-80
One component, silver filled epoxy with a curing temperature of 80°C
Glass Transition Temperature (Tg)
110-120°C
Volume Resistivity
<0.001 ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
10,000-15,000 cps 60-90 minutes at 80°C 75-85 Shore D -76°F to +302°F /tds/ep4s-80
EP4TC-80 One Part Epoxy
EP4TC-80
One component thermally conductive, electrically insulating epoxy with a curing temperature of 80°C
Glass Transition Temperature (Tg)
120-125°C
Thermal Conductivity
11-15 BTU•in/(ft²•hr•°F) [1.6-2.2 W/(m•K)]
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
300,000-800,000 cps 80°C for 90-120 minutes with an optional post cure of 1-2 hours at 80°C 85-95 Shore D -58°F to +347°F /tds/ep4tc-80
EP4UF-80 One Component Epoxy
EP4UF-80
One component epoxy for bonding and underfill applications, minimum curing temperature 80°C
Glass Transition Temperature (Tg)
150-155°C
Volume Resistivity
>10¹⁴ ohm-cm
  • RoHS Compliant
  • NASA Low Outgassing
  • Bonding
  • Underfill
  • Sealing
  • Coating
500-1,500 cps 30-60 minutes at 80-85°C, or 15-30 minutes at 90-95°C 85-95 Shore D -58°F to +302°F /tds/ep4uf-80
EP5LTE-100 is a flowable, one part epoxy with a low coefficient of thermal expansion
EP5LTE-100
One component epoxy for bonding and sealing featuring a low coefficient of thermal expansion and a curing temperature of 100°C
Coefficient of Thermal Expansion
8-12 x 10⁻⁶ in/in/°C
Glass Transition Temperature (Tg)
120-125°C
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
20,000-160,000 cps 90-120 minutes at 100°C followed by 2-3 hours at 100-125°C 85-95 Shore D -76°F to +347°F /tds/ep5lte-100
EP63 One Part Adhesive System
EP63

One component, moderate viscosity epoxy for bonding and sealing that cures at 80°C to 90°C

Glass Transition Temperature (Tg)
140-150°C
Tensile Modulus
350,000-500,000 psi
  • RoHS Compliant
  • Bonding
  • Sealing
35,000-55,000 cps 3-4 hours at 80-90°C followed by post curing at 125°C for 1-2 hours 85-90 Shore D -80°F to +500°F [-62°C to +260°C] /tds/ep63
EP6STC-80
EP6STC-80

One component, highly thermally conductive, silver filled epoxy, cures at 80-90°C

Thermal Conductivity
13-14 W/(m•K)
Volume Resistivity
<0.001 ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
Thixotropic 85-95 Shore D -60°C to +150°C /tds/ep6stc-80
Supreme 10AOHT One Part Epoxy System
Supreme 10AOHT
One component, thermally conductive, electrically insulating, high performance epoxy for bonding and sealing
Tensile Lap Shear Strength
3,400-3,600 psi
Volume Resistivity
>10¹⁴ ohm-cm
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste 250°F for 60-70 minutes, 300°F for 40-50 minutes 80-85 Shore D 4K to +400°F /tds/supreme-10aoht
Supreme 10AOHT-LO One Part Epoxy System
Supreme 10AOHT-LO
One component, thermally conductive, electrically insulating, high performance epoxy for bonding and sealing meets NASA low outgassing specifications
Dielectric Constant
4.3
Tensile Lap Shear Strength
3,400-3,600 psi
  • NASA Low Outgassing
  • 1,000 Hours at 85°C/85% RH
  • RoHS Compliant
  • Bonding
paste 250°F for 60-70 minutes, 300°F for 40-50 minutes 80-90 Shore D 4K to +400°F /tds/supreme-10aoht-lo