Product Certifications Applications Viscosity Cure Schedule Hardness Temp. Range Link to Content
EP21NS Two Component Epoxy
EP21NS
Two part, moderate viscosity, nanosilica filled epoxy system for bonding, sealing, coating and encapsulation
Dielectric Constant
2.8
Refractive Index
1.55
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gap Filling
50,000-90,000 cps overnight at 75°F, followed by 4-5 hours at 150°F 75-85 Shore D -80°F to +250°F /tds/ep21ns
EP21QF Two Component Epoxy
EP21QF
Two component, room temperature curing epoxy featuring easy processing and good physical strength properties
Dielectric Constant
3.4
Dielectric Strength
>450 volts/mil
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gap Filling
20,000-30,000 cps 1 hour at 65°C for 22 grams 75-85 Shore D -80°F to +300°F /tds/ep21qf
EP21SC-1 Two Part Epoxy Compound
EP21SC-1
Two component epoxy resin system for bonding, coating and sealing
Coefficient of Thermal Expansion
21-24 X 10⁻⁶ in/in/°C
Volume Resistivity
>10¹⁴ ohm-cm
  • ASTM D4060-14 for Abrasion Resistance
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste overnight at 75°F plus 2-3 hours at 150-200°F 90-95 Shore D -60°F to +250°F /tds/ep21sc-1
EP21TDC Two Component Epoxy
EP21TDC
Versatile, toughened two component epoxy for bonding, sealing and coating
T-peel Strength
20-30 pli
Volume Resistivity
>10¹⁴ ohm-cm
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
  • Encapsulation
Part A: 11,000-16,000 cps, Part B: 70,000-140,000 cps overnight at 75°F, followed by 1-2 hours at 150-200°F >60 Shore D -100°F to +250°F /tds/ep21tdc
EP21TDC-2 Two Part Epoxy
EP21TDC-2
Two component, highly flexibilized epoxy resin compound
Elongation
>120%
T-peel Strength
>30 pli
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gap Filling
Part A: 10,000-20,000 cps, Part B: 150,000-300,000 cps overnight at 75°F followed by 2-3 hours at 150-200°F 75-80 Shore A 4K to +250°F /tds/ep21tdc-2
EP21TDC-2AO Two Part Epoxy
EP21TDC-2AO
Two component, room temperature curing, thermally conductive, electrically insulative epoxy system
Elongation
50-100%
T-peel Strength
10-20 pli
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
Part A: 30,000-80,000 cps, Part B: 300,000-600,000 cps overnight at 75°F, followed by 2-4 hours at 150-200°F 30-40 Shore D 4K to +250°F /tds/ep21tdc-2ao
EP21TDC-2AOLV Two Part Epoxy Compound
EP21TDC-2AOLV
Two component, room temperature curing, thermally conductive, electrically insulative epoxy system
Elongation
50-100%
T-peel Strength
10-20 pli
  • RoHS Compliant
  • Bonding
  • Sealing
  • Gap Filling
  • Encapsulation
  • Coating
Part A: 1,000-5,000 cps, Part B: 300,000-600,000 cps 75°F: 48-72 hours; 200°F: 2-3 hours 30-40 Shore D 4K to +250°F /tds/ep21tdc-2aolv
EP21TDC-2LOND Two Part Epoxy Compound
EP21TDC-2LOND
Two component, highly flexibilized epoxy resin compound
Tensile Modulus
2,000-7,000 psi
Volume Resistivity
>10¹³ ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
paste 75°F for 48-72 hours, 200°F for 2-3 hours 30-40 Shore D 4K to +250°F /tds/ep21tdc-2lond
EP21TDC-2ND Two Part Epoxy
EP21TDC-2ND
Two component, highly flexibilized, non-drip epoxy resin compound
Dielectric Constant
3.6
Elongation
>120%
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Part A: paste, Part B: paste overnight at 75°F followed by 2-3 hours at 150-200°F 70-80 Shore A 4K to +250°F /tds/ep21tdc-2nd
EP21TDC-4 Two Component Epoxy
EP21TDC-4
Two component, highly flexibilized epoxy for bonding, sealing and coating
Elongation
100-150%
Volume Resistivity
>10¹⁴ ohm-cm
  • 1,000 Hours at 85°C/85% RH
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Part A: 9,000-14,000 cps, Part B: 200,000-300,000 cps 12 hours at 75°F followed by 3-5 hours at 140-160°F 75-85 Shore A -100°F to +250°F /tds/ep21tdc-4