EP29LPHE Two Component Epoxy
EP29LPHE
Two part, very low viscosity epoxy for bonding, sealing, coating and potting
Dielectric Strength
450 volts/mil
Elongation
100-150%
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
350-700 cps 12-24 hours at 75°F, followed by 4-5 hours at 140-180°F 50-60 Shore D -60°F to +250°F /tds/ep29lphe
EP29LPHT Two Part Epoxy System
EP29LPHT
Two part, low viscosity epoxy for bonding, sealing, potting and filament winding featuring higher temperature resistance
Tensile Lap Shear Strength
2,400-2,600 psi
Volume Resistivity
>10¹⁵ ohm-cm
  • RoHS Compliant
  • Bonding
  • Sealing
  • Potting
  • Gap Filling
  • Encapsulation
500-2,000 cps overnight at 75°F followed by 6 to 8 hours at 140-165°F. If possible, post curing for an additional 4 to 6 hours at 150-200°F will enhance the product's properties. 80-90 Shore D -80°F to +350°F /tds/ep29lpht
EP29LPSPAO Two Part Epoxy
EP29LPSPAO
Two component, low viscosity epoxy for bonding, sealing, coating, potting and encapsulation
Tensile Lap Shear Strength
>1,000 psi
Tensile Modulus
>450,000 psi
  • RoHS Compliant
  • MIL-STD-810G for Fungus Resistance
  • Bonding
  • Coating
  • Sealing
  • Potting
  • Encapsulation
  • Casting
4,000-15,000 cps gelling the mixed epoxy at 75°F, followed by alternative lower elevated temperature cure cycles (8-10 hours at 130-150°F) or (5-7 hours at 175°F) or (3-5 hours at 200°F) >75 Shore D 4K to +275°F /tds/ep29lpspao
EP29LPSPAO-1 Black Two Part Epoxy
EP29LPSPAO-1 BLACK
Two component, thermally conductive, electrically insulative, cryogenically serviceable epoxy
Coefficient of Thermal Expansion
22-25 X 10⁻⁶ in/in/°C
Volume Resistivity
>10¹⁵ ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Potting
  • Encapsulation
  • Gap Filling
  • Casting
  • Underfill
4,000-15,000 cps Gel at room temp followed by any option listed below: 130-150°F for 8-10 hours, 175°F for 5-7 hours, 200°F for 3-5 hours 80-85 Shore D 4K to +250°F /tds/ep29lpspao-1-black
EP29LPSPND-3 is a two component epoxy system for use in cryogenic applications
EP29LPSPND-3
Two component epoxy compound for cryogenic applications
Dielectric Constant
4.2
Refractive Index
1.56
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste Gel at 75°F for 12-24 hours followed by either option listed below: 130-150°F for 12-18 hours or 150-165°F for 5-10 hours. 70-80 Shore D 4K to 250°F /tds/ep29lpspnd-3
Two Part Epoxy EP29LPTCHT
EP29LPTCHT
Two component, thermally conductive, electrically insulative epoxy system
Coefficient of Thermal Expansion
22-24 x 10⁻⁶ in/in/°C
Dielectric Constant
4.4
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Encapsulation
  • Potting
  • Underfill
  • Casting
  • Gap Filling
5,000-15,000 cps overnight at 75°F followed by 4-5 hours at 160°-180°F 80-90 Shore D -60°F to +350°F /tds/ep29lptcht
EP30 Two Component Epoxy Adhesive System
EP30
Highly versatile, two part epoxy system for bonding, coating, sealing and casting
Dielectric Strength
440 volts/mil
Refractive Index
1.57
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Potting
Part A: 400-900 cps, Part B: 280-500 cps can be cured at 75°F in 24-48 hours or faster cures can be realized at elevated temperatures, e.g., 2-3 hours at 200°F 80-90 Shore D -60°F to +250°F /tds/ep30
EP30-2LB Two Part Epoxy System
EP30-2LB
Two component, room temperature curing, optically clear epoxy for bonding, sealing, coating and encapsulation. Formulated to have special optical properties
Refractive Index
1.55
Volume Resistivity
>10¹⁵ ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Coating
  • Potting
  • Sealing
  • Encapsulation
  • Gap Filling
Part A: 10,000-16,000 cps, Part B: 10-35 cps 24-48 hours at 75°F or 2-3 hours at 150-200°F 80-90 Shore D -80°F to +300°F /tds/ep30-2lb
EP30-3 Two Part Epoxy Compound
EP30-3
Highly versatile, two part epoxy system for bonding, coating, sealing and casting
Glass Transition Temperature (Tg)
>325°F
Volume Resistivity
>10¹⁵ ohm-cm
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gap Filling
2,000-5,000 cps 60-120 minutes at 170°F plus 2-3 hours at 300°F >75 Shore D -80°F to +450°F /tds/ep30-3
EP30-3LO Two Component Epoxy
EP30-3LO
Highly versatile, two part epoxy system for bonding, coating, sealing and casting
Glass Transition Temperature (Tg)
170-175°C
Volume Resistivity
>10¹⁵ ohm-cm
  • NASA Low Outgassing
  • 1,000 Hours at 85°C/85% RH
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Casting
  • Encapsulation
  • Gap Filling
2,000-5,000 cps 1-2 hours at 170°F followed by 2-3 hours at 300°F 80-90 Shore D -80°F to +450°F /tds/ep30-3lo