Product Certifications Applications Viscosity Cure Schedule Hardness Temp. Range Link to Content
EP45HTMed Two Part Epoxy System
EP45HTMed
Two component, high temperature resistant, medical grade epoxy resists repeated sterilizations
Glass Transition Temperature (Tg)
150-160°C
Volume Resistivity
>10¹⁴ ohm-cm
  • USP Class VI Medical
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Casting
  • Encapsulation
  • Gap Filling
  • Potting
50,000-60,000 cps 250°F for 3-4 hours or 300°F for 2-3 hours 75-85 Shore D -80°F to 500°F /tds/ep45htmed
EP45HTND-2 Two Component Epoxy System
EP45HTND-2
Two component epoxy system for high performance bonding, sealing and coating
Dielectric Constant
4.3
Glass Transition Temperature (Tg)
150-160°C
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gap Filling
Part A: paste, Part B: paste 3-4 hours at 250°F or 2-3 hours at 300°F 75-85 Shore D -80°F to +500°F /tds/ep45htnd-2
EP46HT Two Part Epoxy
EP46HT
Two component, heat resistant epoxy system for bonding and sealing
Dielectric Strength
450 volts/mil
Glass Transition Temperature (Tg)
175°C
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gap Filling
3,000-6,000 cps 250-300°F for 3-4 hours >80 Shore D -80°F to +500°F /tds/ep46ht
EP46HT-1 Two Part Epoxy Compound
EP46HT-1
Two component epoxy for structural bonding featuring superlative heat resistance; requires oven curing
Dielectric Strength
450 volts/mil
Glass Transition Temperature (Tg)
230-240°C
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
15,000-35,000 cps 250-300°F for 2-3 hours, followed by a post cure for optimum properties at 350-400°F for 2 hours 80-90 Shore D -100°F to +600°F /tds/ep46ht-1
EP46HT-1ND2 Two Part Epoxy System
EP46HT-1ND-2
Two component epoxy paste for structural bonding featuring superlative heat resistance; requires oven curing. Will not flow during processing
Dielectric Strength
450 volts/mil
Tensile Lap Shear Strength
>2,200 psi
  • RoHS Compliant
  • Bonding
  • Sealing
  • Gap Filling
  • Coating
paste 250-300°F for 2-3 hours, followed by a post cure for optimum properties at 350-400°F for 2 hours 80-90 Shore D -100°F to +600°F /tds/ep46ht-1nd-2
EP46HT-2 Two Part Epoxy
EP46HT-2
Two part high performance epoxy for bonding, sealing, coating and casting
Dielectric Strength
450 volts/mil
Glass Transition Temperature (Tg)
155-165°C
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
  • Sealing
  • Coating
  • Casting
12,000-20,000 cps 250-300°F, 3-4 hours 80-90 Shore D -100°F to +500°F /tds/ep46ht-2
EP46HT-2AO Black Two Part Epoxy
EP46HT-2AO Black
Two part high performance epoxy for bonding, sealing and encapsulation
Dielectric Strength
450 volts/mil
Volume Resistivity
>10¹⁴ ohm-cm
  • MIL-STD-810G for Fungus Resistance
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Encapsulation
  • Coating
  • Casting
  • Potting
  • Gap Filling
140,000-280,000 cps 3-4 hours at 250-300°F followed by a post cure of 2-3 hours at 350-400°F 85-90 Shore D -100°F to +500°F /tds/ep46ht-2ao-black
EP46HT-2Med Two Component Epoxy
EP46HT-2Med
Two component, heat resistant, medical grade epoxy
Dielectric Strength
450 volts/mil
Tensile Strength
10,000-11,000 psi
  • USP Class VI Medical
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Potting
  • Encapsulation
  • Gap Filling
12,000-20,000 cps 250-300°F for 3-4 hours, followed by 350-400°F for 2-3 hours 80-90 Shore D -100°F to +500°F /tds/ep46ht-2med
EP46HT-2ND2 Two Part Epoxy Compound
EP46HT-2ND2
Two part, non-drip epoxy for bonding, sealing, coating and casting
Glass Transition Temperature (Tg)
155-165°C
Tensile Modulus
400,000-450,000 psi
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
paste 250-300°F: 3-4 hours; post cure, 350-400°F: 2-3 hours 80-90 Shore D -100°F to +500°F /tds/ep46ht-2nd2
EP48TC Two Part Epoxy Adhesive
EP48TC
Two part epoxy adhesive with ultra low thermal resistance properties meets NASA low outgassing requirements
Coefficient of Thermal Expansion
13-15 X 10⁻⁶ in/in/°C
Dielectric Constant
4.7
Volume Resistivity
>10¹⁴ ohm-cm
  • NASA Low Outgassing
  • 1,000 Hours at 85°C/85% RH
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste overnight at 75°F followed by 3-5 hours at 150-200°F 85-95 Shore D -100°F to +300°F /tds/ep48tc