UV15DC80-10FHC UV and heat curable epoxy formulation. Cures in "shadowed out" areas at temperatures as low as 80°C. Convenient no mix system. Serviceable from -60°F to +350°F. Superb electrical insulator. Low to moderate viscosity system. |
|
UV15DC80-1Med UV and heat curable epoxy formulation. Cures in "shadowed out" areas at temperatures as low as 80°C. Meets ISO 10993-5. Convenient no mix system. Serviceable from -80°F to +350°F. Superb electrical insulator. |
|
UV15DC80-FHC UV and heat curable epoxy formulation. Cures in "shadowed out" areas at temperatures as low as 80°C. Passes 1,000 hours at 85°C/85% humidity. Convenient no mix system. Serviceable from -60°F to +350°F. Superb electrical insulator. |
|
UV15DC80LV UV and/or heat curable modified epoxy resin system. One component 100% reactive adhesive, sealant, coating. Thermal cure at 80°C for 40-60 minutes. High bond strength. Resists moisture and chemical exposure. Serviceable up to 350°F. |
|
UV15DC80LV-FHC UV and/or heat curable modified epoxy resin system. One component 100% reactive adhesive, sealant, coating. Thermal cure at 80°C for 40-60 minutes. High bond strength. Resists moisture and chemical exposure. Serviceable up to 350°F. |
|
UV15DC80Med USP Class VI approved one component UV and heat curable epoxy. Passes ISO 10993-5 cytotoxicity testing. Cures at temperatures as low as 80°C. Moderate viscosity. Minimal shrinkage upon cure. Capable of withstanding liquid sterilants, radiation, autoclaving. Serviceable from -60°F to +400°F. |
|
UV15DC80ND UV and heat curable epoxy formulation. Cures in "shadowed out" areas at temperatures as low as 80°C. Passes 1,000 hours at 85°C/85% humidity. Convenient no mix system. Serviceable from -60°F to +350°F. Superb electrical insulator. |
|
UV15DC80TK UV and heat curable epoxy formulation. Cures in "shadowed out" areas at temperatures as low as 80°C. Passes 1,000 hours at 85°C/85% humidity. Convenient no mix system. Serviceable from -60°F to +350°F. Superb electrical insulator. |
|
UV15FL Low viscosity epoxy system with enhanced toughness. Substantial temperature resistance, especially when post cured with heat. 100% reactive. Shore D hardnes >75. Tensile strength >5,000 psi. Optically clear, spin coatable. Serviceable from -80°F to +350°F. |
|
UV15LV Low viscosity, high strength epoxy resin based formulation. Enhanced thermal stability. Cationic curing system. Excellent light transmission properties. Superb electrical insulation characteristics. Serviceable from -80°F to +300°F. |