MasterSil 705TC Thermally conductive and electrically isolating. Easy to use silicone for high performance bonding, sealing and coating. Non-corrosive and room temperature curable. Ideally suited for applications requiring flexibility and high temperature resistance. |
|
|
MasterSil 972TC-LO Thermally conductive, electrically insulative bonding, potting, sealing formulation. NASA low outgassing approved. Long working life after mixing. Can cure in thick and wide sections. Good flexibility and elongation. Serviceable from -120°F to +400°F. |
|
|
MasterSil 973S-LO Silver filled, two part, addition cured type silicone. Excellent electrical conductivity. Passes NASA low outgassing test requirements. Highly flexible. Service temperature range from -120°F to +400°F. Volume resistivit >0.004 ohm-cm. |
|
MB600G Graphite filled, aqueous based, sodium silicate based coating for EMI/RFI shielding and static dissipation. Cost effective. Easily applied by brush or spraying. Superb temperature resistance from 0°F to +700°F. |
|
MB600S Aqueous based sodium silicate system. One component, silver filled formulation. Highly effective moisture barrier. Bonds well to a wide variety of substrates. Temperature resistance up to 700°F. Excellent shielding effectiveness. Simple, safe handling. |
|
MB600SCN Electrically conductive sodium silicate, aqueous based coating. Silver coating nickel filled system. Impressive shielding effectiveness Room temperature or heat curable. Can be effectively brushed or sprayed on surfaces. Serviceable from 0°F to +700°F. |
|
Super Gel 9AO Thermally conductive/electrically insulative urethane modified epoxy system. Soft and resilient. Solid dimensional stability. Easily repairable. Long working life. Low exotherm. Service temperature range -100°F to +200°F. Superior electrical insulation properties. Can be cast many inches in depth. Withstands thermal cycling and mechanical shock. |
|
Super Gel 9AOND Two component urethane modified epoxy system. Exceptionally soft. Shore A hardness 20-30. Retains dimensional stability. Thermally conductive/electrically insulative. Non-drip paste. Service temperature range -100°F to +200°F. Ideal for bonding/sealing. Easily repairable. |
|
Supreme 10ANHT Thermally conductive version of our one part Supreme 10HT epoxy system with excellent heat transfer properties. Outstanding bond strength. Thermal conductivity 20-25 BTU ·in/ft2 ·hr/°F. Serviceable from 4k to +400°F. Superior durability. Versatile cure schedule at elevated temperatures. Can withstand prolonged exposure to water, fuels, oil, organic solvents. Gray color. |
|
Supreme 10ANHT-LO NASA low outgassing approved one component thermally conductive epoxy adhesive. Cryogenically serviceable. Smooth paste consistency. Low coefficient of thermal expansion. Effective shear and peel strength. Stellar electrical insulation properties. Serviceable from 4K to +400°F. |