 EP21FL Two Part Epoxy
EP21FL
Toughened, two component epoxy for bonding, sealing and encapsulation
Tensile Modulus
150,000-200,000 psi
Volume Resistivity
10¹⁴ ohm-cm
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gap Filling
  • Potting
2,000-4,500 cps Optimum cure schedule: overnight at 75°F plus 2-3 hours at 150-200°F 40-50 Shore D -100°F to +250°F /tds/ep21fl
EP21FRNS-2 Two Component Epoxy System
EP21FRNS-2
Two component epoxy system for potting, encapsulating and casting
Dielectric Constant
4.5
Tensile Lap Shear Strength
>1,200 psi
  • RoHS Compliant
  • UL 94V-0 Flame Resistant
  • Casting
  • Encapsulation
  • Potting
  • Sealing
Part A: 40,000-70,000 cps, Part B: 30,000-45,000 cps Cures at 75°F, 48-72 hours >75 Shore D -59.8°F to +194°F /tds/ep21frns-2
EP21H Two Component, Optically Clear Epoxy
EP21H
Two component epoxy compound for high performance applications
Refractive Index
1.54
Volume Resistivity
>10¹⁴ ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Potting
  • Casting
3,000-6,000 cps 12-24 hours at 75°F, plus 3-4 hours at 150°F >75 Shore D -60°F to +250°F /tds/ep21h
EP21HT Two Part Epoxy System
EP21HT
Two component epoxy compound for high performance applications
Dielectric Constant
2.90
Tensile Lap Shear Strength
>3,000 psi
  • FDA Food Grade 21 CFR 175.105
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gap Filling
Part A: 60,000-110,000 cps, Part B: 11,000-15,000 cps Cures within 48-72 hours at 75°F >75 Shore D -60°F to +400°F /tds/ep21ht
EP21HT-LO Two Part Epoxy System
EP21HT-LO
Two component epoxy compound for high performance applications
Tensile Lap Shear Strength
2,800-3,000 psi.
Volume Resistivity
>10¹⁴ ohm-cm.
  • NASA Low Outgassing
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
  • Sealing
  • Coating
Part A: 60,000-110,000 cps., Part B: 11,000-15,000 cps. 75°F: 48-72 hours; 200°F: 2-3 hours; Optimum cure schedule: overnight at 75°F, followed by 2 hours at 150-200°F. 75-85. Shore D -60°F to +400°F. /tds/ep21ht-lo
EP21HTFG Two Component Epoxy System
EP21HTFG
Two component epoxy compound for high performance applications
Tensile Lap Shear Strength
>3,000 psi.
Volume Resistivity
>10¹⁴ ohm-cm.
  • RoHS Compliant
  • FDA Food Grade 21 CFR 175.105
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Part A: 60,000-110,000 cps., Part B: 11,000-15,000 cps. Cures within 48-72 hours at 75°F. >75 Shore D -60°F to +400°F. /tds/ep21htfg
EP21HTND Two Component Epoxy Adhesive
EP21HTND
Two component epoxy compound for bonding, sealing and coating
Dielectric Constant
2.90
Volume Resistivity
>10¹⁴ ohm-cm
  • FDA Food Grade 21 CFR 175.105
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
Part A: paste, Part B: paste Cures readily at 75°F or faster at elevated temperatures with the optimum being overnight at 75°F followed by 1-2 hours at 150-200°F. >75 Shore D -60°F to +400°F /tds/ep21htnd
EP21LSCL-2 Two Part Epoxy
EP21LSCL-2
Two component, optically clear epoxy for bonding, coating, sealing and potting featuring superior non-yellowing properties and temperature resistance
Dielectric Strength
440 volts/mil
Refractive Index
1.57
  • RoHS Compliant
  • NASA Low Outgassing
  • Bonding
  • Sealing
  • Coating
  • Potting
  • Casting
  • Gap Filling
  • Encapsulation
Part A: 1,500 - 2,500 CPS, Part B: 5 - 50 CPS overnight at 75°F followed by 3-5 hours at 140-175°F 80-90 Shore D -60°F to +350°F /tds/ep21lscl-2
Two Part Epoxy EP21LSCL-2Med
EP21LSCL-2Med
Two component, optically clear epoxy for bonding, coating, sealing and potting featuring superior non-yellowing properties
Dielectric Strength
440 volts/mil
Refractive Index
1.57
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Potting
  • Encapsulation
  • Gap Filling
  • Underfill
600-900 cps overnight at 75°F followed by 3-5 hours at 140-175°F 80-90 Shore D -60°F to +350°F /tds/ep21lscl-2med
EP21LV Two Component Low Viscosity Epoxy System
EP21LV
Two component, low viscosity epoxy compound
Dielectric Strength
440 volts/mil
Tensile Lap Shear Strength
>2,800 psi
  • FDA Food Grade 21 CFR 175.105
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Casting
  • Encapsulation
10,000-13,000 cps 75°F: 24-48 hours >70 Shore D -65°F to +250°F /tds/ep21lv