FL901S Epoxy Based Film FL901S

High performance, silver filled epoxy adhesive film system with outstanding electrical and thermal conductivity. Superior mechanical strength, convenient handling, good storage stability and fast cures at moderate temperatures. Specialty preforms are available. Serviceable from -100°F to +500°F.

MasterSil 151S Two Part Silicone System MasterSil 151S

Addition curing, two part silicone for use as an adhesive, sealant, coating or form-in-place gasketing material. Despite its silicone chemistry, it passes NASA low outgassing specifications. It is ideal for applications where low stress is required.

MasterSil 155 Two Part Silicone System MasterSil 155

Two part, graphite filled silicone adhesive. Convenient one to one mix ratio by weight. Volume resistivity 20-40 ohm-cm. Elongatio >300%. Serviceable from -85°F to +400°F.

MasterSil 705C One Part Silicone MasterSil 705C

Single component, electrically conductive, non-corrosive silicone compound. Carbon filled. Tack free time 3-7 minutes at ambient temperatures. Paste viscosity. Serviceable up to 400°F.

MastersSil 705S One Component Silicone MasterSil 705S

Silver filled, one-part, no-mix, non-corrosive silicone system. Shore A hardness 70. Cures at room temperatures when exposed to atmospheric moisture. Extremely low volume resistivity. Most effective when applied in thin sections.

MasterSil 973S-LO Two Part Silicone Compound MasterSil 973S-LO

Silver filled, two part, addition cured type silicone. Excellent electrical conductivity. Passes NASA low outgassing test requirements. Highly flexible. Service temperature range from -120°F to +400°F. Volume resistivit >0.004 ohm-cm.

MB600S One Part Sodium Silicate System MB600S

Aqueous based sodium silicate system. One component, silver filled formulation. Highly effective moisture barrier. Bonds well to a wide variety of substrates. Temperature resistance up to 700°F. Excellent shielding effectiveness. Simple, safe handling.

MB600SCN One Part Sodium Silicate Coating MB600SCN

Electrically conductive sodium silicate, aqueous based coating. Silver coating nickel filled system. Impressive shielding effectiveness Room temperature or heat curable. Can be effectively brushed or sprayed on surfaces. Serviceable from 0°F to +700°F.

Supreme 10HTN One Part Epoxy Supreme 10HTN-NV

High peel and shear strength single component nickel filled epoxy adhesive. Thixotropic system. Cost effective electrical conductivity. Resists from 4k to +400°F.

Supreme 10HTS One Part Epoxy Supreme 10HTS

Silver filled system with excellent electrical conductivity and high physical strength properties. One part, heat cured (250-300°F) epoxy. Wide range of serviceability from cryogenic temperatures up to +400°F. Meets NASA low outgassing specifications. Can be applied without sagging or dripping, even on vertical surfaces. Volume resistivit <0.006 ohm-cm. Thermally conductive. Shore D hardnes >75.