Product Selector

Filters
Applications
Product Type
Certifications
Thermal Conductivity
Product Certifications Applications Viscosity Cure Schedule Hardness Temp. Range Link to Content
EP21TDC Two Component Epoxy
EP21TDC
Versatile, toughened two component epoxy for bonding, sealing and coating
T-peel Strength
20-30 pli
Volume Resistivity
>10¹⁴ ohm-cm
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
  • Encapsulation
Part A: 11,000-16,000 cps, Part B: 70,000-140,000 cps overnight at 75°F, followed by 1-2 hours at 150-200°F >60 Shore D -100°F to +250°F /tds/ep21tdc
EP21TDC-2 Two Part Epoxy
EP21TDC-2
Two component, highly flexibilized epoxy resin compound
Elongation
>120%
T-peel Strength
>30 pli
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gap Filling
Part A: 10,000-20,000 cps, Part B: 150,000-300,000 cps overnight at 75°F followed by 2-3 hours at 150-200°F 75-80 Shore A 4K to +250°F /tds/ep21tdc-2
EP21TDC-2AO Two Part Epoxy
EP21TDC-2AO
Two component, room temperature curing, thermally conductive, electrically insulative epoxy system
Elongation
50-100%
T-peel Strength
10-20 pli
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
Part A: 30,000-80,000 cps, Part B: 300,000-600,000 cps overnight at 75°F, followed by 2-4 hours at 150-200°F 30-40 Shore D 4K to +250°F /tds/ep21tdc-2ao
EP21TDC-2AOLV Two Part Epoxy Compound
EP21TDC-2AOLV
Two component, room temperature curing, thermally conductive, electrically insulative epoxy system
Elongation
50-100%
T-peel Strength
10-20 pli
  • RoHS Compliant
  • Bonding
  • Sealing
  • Gap Filling
  • Encapsulation
  • Coating
Part A: 1,000-5,000 cps, Part B: 300,000-600,000 cps 75°F: 48-72 hours; 200°F: 2-3 hours 30-40 Shore D 4K to +250°F /tds/ep21tdc-2aolv
EP21TDC-2LOND Two Part Epoxy Compound
EP21TDC-2LOND
Two component, highly flexibilized epoxy resin compound
Tensile Modulus
2,000-7,000 psi
Volume Resistivity
>10¹³ ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
paste 75°F for 48-72 hours, 200°F for 2-3 hours 30-40 Shore D 4K to +250°F /tds/ep21tdc-2lond
EP21TDC-2ND Two Part Epoxy
EP21TDC-2ND
Two component, highly flexibilized, non-drip epoxy resin compound
Dielectric Constant
3.6
Elongation
>120%
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Part A: paste, Part B: paste overnight at 75°F followed by 2-3 hours at 150-200°F 70-80 Shore A 4K to +250°F /tds/ep21tdc-2nd
EP21TDC-4 Two Component Epoxy
EP21TDC-4
Two component, highly flexibilized epoxy for bonding, sealing and coating
Elongation
100-150%
Volume Resistivity
>10¹⁴ ohm-cm
  • 1,000 Hours at 85°C/85% RH
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Part A: 9,000-14,000 cps, Part B: 200,000-300,000 cps 12 hours at 75°F followed by 3-5 hours at 140-160°F 75-85 Shore A -100°F to +250°F /tds/ep21tdc-4
EP21TDC-4ND Two Part Epoxy
EP21TDC-4ND
Two component, highly flexibilized epoxy for bonding, sealing and coating
Elongation
100-200%
Tensile Lap Shear Strength
>850 psi
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste overnight at 75°F followed by 3-4 hours at 150-200°F 75-80 Shore A -100°F to +250°F /tds/ep21tdc-4nd
EP21TDC-7 Two Component Epoxy
EP21TDC-7
Two component, highly flexibilized epoxy for bonding, sealing and coating
Elongation
>200%
Volume Resistivity
>10¹⁴ ohm-cm
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
Part A: 9,000-14,000 cps, Part B: 200,000-300,000 cps 12 hours at 75°F followed by 3-5 hours at 140-160°F 65-75 Shore A -100°F to +250°F /tds/ep21tdc-7
EP21TDCAOHT Two Part Epoxy
EP21TDCAOHT
Two component epoxy compound for bonding, sealing and coating
Coefficient of Thermal Expansion
21-24 X 10⁻⁶ in/in/°C
Tensile Lap Shear Strength
1,000-1,200 psi
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Part A: 100,000-400,000 cps, Part B: paste Optimum cure schedule: overnight at 75°F, plus 2-4 hours at 150-200°F. 85-95 Shore D -100°F to +250°F /tds/ep21tdcaoht

Need Expert Guidance?