Bonding substrates with widely different thermal expansion coefficients, such as glass and aluminum or plastics and ceramics, can be readily accomplished with properly selected adhesive compositions. Adhesives with compliant bond characteristics are the key for achieving high strength, durable bonds between such substrates.