Master Bond LED422DC90 is a one component, nanosilica filled dual cure adhesive system engineered for high-speed fixturing and bonding of opaque substrates.
This unique "side-bonding" capability allows for rapid polymerization up to 3-4 mm in depth by exposing the adhesive to 405 nm LED light from an angle.
Master Bond EP3HTSDA-2Med is a true one component epoxy that is not pre-mixed and frozen. It offers an easy dispensing profile with an exceptionally long working life at room temperature, making it ideal for streamlining automated assembly. As a silver filled system, it exhibits high electrical conductivity (volume resistivity < 0.001 ohm-cm) and excellent thermal conductivity.
Master Bond UV15-7HP is a low viscosity, easy to apply, one-part, UV curable adhesive system.
Optimal adhesion is achieved in bond line thicknesses of 0.001-0.003 inch, and it can cure rapidly with a minimum intensity of 20-40 milliwatts/cm2 using a
Master Bond EP29LPSPND-3 is a two component, non-drip epoxy compound with a paste consistency that can be used for bonding and sealing applications. The system is electrically non-conductive and thermally insulative, with a thermal conductivity of approximately 0.2 W/(m•K) at room temperature. It withstands cryogenic temperatures and is serviceable in the range from 4K to 250°F.
Master Bond LED415DC90Med is a one component, dual cure adhesive system designed for high-speed manufacturing of medical electronic devices. It cures rapidly without oxygen inhibition upon exposure to 405 nm LED light, followed by a short 30-45 minute heat cure at 90-95°C, making it well-suited for bonding heat sensitive components.
Master Bond has launched EP53TC, a two-component epoxy designed for bonding, sealing, coating, and small potting applications where efficient heat dissipation is crucial. The epoxy is formulated with a specialty filler with a particle size ranging from 5 to 30 microns. It is a flowable system with a mixed viscosity of 45,000-65,000 cps at room temperature.
 
			      