Master Bond EP41S-5Med is a two part epoxy system that meets the requirements of ISO 10993-5 for non-cytotoxicity
and can be used for bonding, sealing, and coating in medical devices. It features high temperature resistance
and good strength properties. As an electrically insulative material, it can be utilized in medical electronic applications.

Master Bond Supreme 42HT-2ND Black is a two-part, non-drip epoxy system designed for bonding, sealing and coating applications.
It is capable of withstanding temperatures up to 450°F (232°C), and provides a glass transition temperature (Tg) of 130-135°C.

Master Bond EP5TC-80 is a one part, NASA low outgassing rated epoxy that achieves a thermal conductivity of 3.3-3.7 W/(m·K),
while also retaining its electrical non-conductivity. It requires a cure at only 80°C for 1.5 to 2 hours.
To optimize performance properties a post cure of 1-2 hours at 80°C is recommended.

Master Bond MasterSil 323AO-LO is a two component silicone elastomer with a self-priming feature, designed for bonding, sealing and gap filling applications.
This electrically insulating and thermally conductive compound meets NASA low outgassing specifications and can be used in the
aerospace, electronic, opto-electronic and specialty OEM industries.

Master Bond EP4CL-80Med is a one part, optically clear epoxy developed for use in medical device assembly applications.
It withstands repeated sterilization cycles and passes ISO 10993-5 testing for non-cytotoxicity.
This product cures at moderate temperatures of around 80-85°C within 60 to 90 minutes and faster at slightly higher temperatures.

Master Bond EP40ND is a two component epoxy system, designed for bonding, sealing and coating applications.
It is a non-drip, toughened system with an easy to use 1:1 mix ratio by weight or volume. EP40ND meets NASA low outgassing specifications and has a high elongation of 80-90% at 75°F.