Master Bond EP42HT-4AOMed Black is a new two part epoxy created for medical device manufacturing.
It is biocompatible and non-cytotoxic, passing both USP Class VI and ISO 10993-5 certifications.
This epoxy withstands aggressive chemical sterilants, radiation and repeated cycles of autoclaving.

Master Bond EP36FR is a specialized one part epoxy that meets Airbus specifications for toxic gas emissions per AITM 3.0005, Issue 2 in the flaming mode
and Section 7.4 of ABD0031, Issue F. It also passes the 12 second vertical burn test per AITM 2.0002B and Section 7.1.2 of ABD0031, Issue F.

EP42-2LV Black is a two part epoxy with low viscosity and good flow. It withstands prolonged immersion in many acids, bases, solvents, fuels and oils.
This versatile system can be used for bonding, sealing, coating and casting, where a strong chemical resistance profile is required.

Master Bond EP40Med, a two part epoxy system, combines toughness and a low tensile modulus while still providing a relatively high lap shear strength.
It meets the requirements of ISO 10993-5 testing and is therefore considered to be non-cytotoxic. This compound can be used for bonding, sealing, coating and encapsulating.

Master Bond EP35SP is a two part epoxy system for bonding and sealing applications, providing resistance to many chemicals such as oils, acids, bases, water, fuels, and especially petrochemicals.

Master Bond EP17HTS-DA is a new one component, no mix, die attach epoxy that is electrically conductive and withstands high temperatures.
It is a silver filled system. Typically, glass transition temperature (Tg) declines with the addition of a filler like silver.