MB250NT One Part Ethyl Cyanoacrylate System MB250NT

Low viscosity ethyl cyanoacrylate. Rapid curing at room temperature; usually sets up within 40 seconds. Passes ISO 10993-5 for cytotoxicity. Resistant to EtO and gamma sterilization. Serviceable from -60°F to +250°F.

MB295 Cyanoacrylate Adhesive MB295

Transparent adhesive. Shore A hardness 85. Bonds well to metals, plastics, glass, rubbers. Fast curing. Viscosity 1,300 to 1,700 cps.

MB297 One Part Ethyl Cyanoacrylate System MB297

Higher viscosity (2,200-2,400 cps) and a slightly longer open time than low viscosity counterparts. High strength, rapid curing ethyl cyanoacrylate system. No heating or mixing needed. Good resistance to cleaning agents. Serviceable from -60°F to +250°F.

MB297FL

Flexibilized cyanoacrylate adhesive offers improved resistance to vibration.1,500-1,800 cps viscosity. Serviceable from -65°F to +185°F.

MB297Med One Part Ethyl Cyanoacrylate Compound MB297Med

Fast setting. Viscosity 2,000 - 2,400 cps. Biocompatible. Resists EtO and gamma sterilization. Passes USP Class VI testing. Bonds well to metals, plastics, rubbers, glass. Serviceable from -60°F to +250°F.

MB297Med-1 One Part Ethyl Cyanoacrylate Adhesive MB297Med-1

Moderate viscosity 1,000-1,100 cps. Rapid curing. Meets USP Class VI specifications. For disposable and reusable medical devices. Serviceable from -60°F to +250°F.

MB297Med-2 One Part Ethyl Cyanoacrylate Compound MB297Med-2

Fast setting. Low viscosity 100-110 cps. Meets USP Class VI specifications. For disposable and reusable medical devices. Serviceable from -60°F to +250°F.

MB297Med-3 Single Component Ethyl cyanoacrylate MB297Med-3

High bond strength. Rapid fixture time. Ultra low viscosity 10-20 cps. USP Class VI approved. For disposable and reusable medical devices. Serviceable from -60°F to +250°F.

MB302 Cyanoacrylate Adhesive MB302

Colorless, transparent low viscosity no mix adhesive. Refractive index 1.46. Recommended for bonding plastics, rubbers, ceramics, metals, glass. High tensile shear strength. Rapid curing.

MB306 One Part Ethyl Cyanoacrylate System MB306

Low viscosity methyl cyanoacrylate with superior bonding properties especially to metals. Contact pressure usually sufficient for fixturing. Viscosity 75-95 cps. Shore D hardness 70. Fast curing. Serviceable from -60°F to +250°F.