MasterSil 930 One Part Fluorosilicone System MasterSil 930

Acetoxy type fluorosilicone for bonding, sealing, coating. Enhanced resistance to fuels, oils, solvents, water, greases. Paste viscosity. Withstands thermal cycling. Serviceable up to +450°F. No mix system.

MasterSil 970-LO Two Part Silicone Compound MasterSil 970-LO

Moderate viscosity, two component silicone adhesive, sealant, encapsulant. Passes NASA low outgassing test requirements. Vacuum compatible. Withstands rigorous thermal cycling and shock. White color. Good flow properties. Serviceable from -120°F to +400°F.

MasterSil 971-LO Two Part Epoxy MasterSil 971-LO

Meets ASTM E595 specifications for low outgassing. Optically clear, two part system with one to one mix ratio by weight. Serviceable from -120°F to +400°F. First class electrical insulator.

MasterSil 972TC-LO Two Part Silicone System MasterSil 972TC-LO

Thermally conductive, electrically insulative bonding, potting, sealing formulation. NASA low outgassing approved. Long working life after mixing. Can cure in thick and wide sections. Good flexibility and elongation. Serviceable from -120°F to +400°F.

MasterSil 980 Two Part Fluorosilicone Compound MasterSil 980

Two part, fluorosilicone for bonding, sealing, coating. Enhanced chemical resistance. Withstand exposure to gasoline, diesel fuel, motor oil, ethanol. Serviceable from -85°F to +465°F. Cures well in wide and deep sections. Moderate viscosity.

MB250NT One Part Ethyl Cyanoacrylate System MB250NT

Low viscosity ethyl cyanoacrylate. Rapid curing at room temperature; usually sets up within 40 seconds. Passes ISO 10993-5 for cytotoxicity. Resistant to EtO and gamma sterilization. Serviceable from -60°F to +250°F.

MB295 Cyanoacrylate Adhesive MB295

Transparent adhesive. Shore A hardness 85. Bonds well to metals, plastics, glass, rubbers. Fast curing. Viscosity 1,300 to 1,700 cps.

MB297 One Part Ethyl Cyanoacrylate System MB297

Higher viscosity (2,200-2,400 cps) and a slightly longer open time than low viscosity counterparts. High strength, rapid curing ethyl cyanoacrylate system. No heating or mixing needed. Good resistance to cleaning agents. Serviceable from -60°F to +250°F.

One Part Cyanoacrylate MB297FLNT MB297FLNT

Low viscosity ethyl cyanoacrylate. Rapid curing at room temperature; usually sets up within 40 seconds. Passes ISO 10993-5 for cytotoxicity. Resistant to EtO and gamma sterilization. Serviceable from -60°F to +250°F.

MB297Med One Part Ethyl Cyanoacrylate Compound MB297Med

Fast setting. Viscosity 2,000 - 2,400 cps. Biocompatible. Resists EtO and gamma sterilization. Passes USP Class VI testing. Bonds well to metals, plastics, rubbers, glass. Serviceable from -60°F to +250°F.