EP42HT-2FG Two Part Epoxy System EP42HT-2FG

Food grade epoxy system toxicologically evaluated to meet the NSF/ANSI 51.4.1 (2009) standard for food equipment materials. Certified to meet FDA CFR 175.300. Excellent resistance to fats, oils, acids, alkalis and many solvents. Withstands boiling water, radiation, chemicals, steam and frozen storage conditions. Strong bonds to similar/dissimilar substrates. Service temperature range -60°F to +450°F. Low viscosity.

EP42HT-2HV1 Two Part Epoxy EP42HT-2HV1

Chemical resistant, two component, room temperature curable epoxy. Serviceability from -60°F to +450°F. Withstands exposure acids, alkalis, solvents, sterilants such as radiation, steam, EtO. Post curing is recommended to optimize properties. Castable to thicknesses exceeding 2-3 inches.

EP42HT-2LO Two Part Epoxy System EP42HT-2LO

NASA low outgassing approved epoxy for service from -60°F to 450°F. Cures at ambient temperatures. Tensile strength >12,000 psi. Shore D hardness 80-90. Superior dimensional stability. Remarkable chemical resistance. Withstands 1,000 hours 85°C/85% RH. Castable in thicknesses exceeding 2-3 inches. Vacuum compatible.

EP42HT-2LTE Two Component Epoxy Compound EP42HT-2LTE

Ultra low coefficient of thermal expansion. Two component, room temperature curing epoxy. Reliable electrical insulator. Unsurpassed dimensional stability. Low linear and volumetric shrinkage upon cure. Serviceable from -60°F to +300°F. Withstands 1,000 hours 85°C/85% RH.

EP42HT-2Med Two Part Epoxy System EP42HT-2Med Black

USP Class VI approved. Serviceable from -60°F to 450°F. Withstands multiple cycles of medical sterilization including radiation, EtO, autoclaving and chemical sterilants. Shore D hardnes >75. Used for bonding, sealing, coating, casting. Can be cured up to 2-3 inches thick. Cures at ambient temperature or more quickly at elevated temperatures.

EP42HT-2Med Black Two Part Epoxy EP42HT-2Med

Low viscosity, two part epoxy with outstanding chemical resistance. Passes USP Class VI biocompatibility tests. Capable of withstanding repeated sterilization cycles including radiation, EtO, chemical sterilants, autoclaving. Serviceable from -60°F to +450°F. Cures at room or elevated temperatures. Available in amber-clear and black colors. Castable in thicknesses up to 2-3 inches.

EP42HT-2ND-2

Serviceable from -60°F to 450°F. Cures at ambient temperatures, or faster with heat. Tensile strength 10,000-11,000 psi. Shore D hardness 80-90. Superior dimensional stability. Remarkable chemical resistance.

EP42HT-2ND-2Med Black Two Part Epoxy System EP42HT-2ND-2Med Black

Two component epoxy paste adhesive. Resists sterilization exposure. USP Class VI approved. Outstanding thermal stability and electrical insulation properties. Cures at ambient temperatures. Withstands multiple cycles of autoclaving, radiation, EtO and chemical sterilants. Post curing is recommended to optimize physical properties. Serviceable from -60°F to +450°F.

EP42HT-3AO Two Part Epoxy EP42HT-3AO

Thermally conductive, electrically insulative. Ideal for potting and encapsulation. Castable up to 3-4 inches. Excellent chemical resistance. Enhanced thermal cycling capabilities. Good flow. Serviceable from -100°F to +400°F. Impervious to intermittent exposures to steam. Shore D hardnes >80.

EP42HT-4AOMed Black Two Component Epoxy EP42HT-4AOMed Black

Thermally conductive, electrically insulative two part epoxy. Meets USP Class VI and ISO 10993-5 certifications. Cryogenically serviceable from 4K to +400F. NASA low outgassing aproved. Black in color. For bonding, sealing, coating and casting.