Supreme 45HTQ Two Part Epoxy Compound Supreme 45HTQ

Two component, toughened, quartz filled epoxy with exceptional abrasion resistance. Heat curing system. Long working life after mixing. High compressive strength. Superb dimensional stability. Serviceable from -60°F to +450°F. Withstands exposure to petrochemicals acids, bases, solvents. Good strength retention at elevated temperatures. Successfully tested for 1,000 at 85°C/85% RH.

Supreme 45HTQ Two Component Epoxy Supreme 45HTQ-4

Toughened, two component silicon carbide filled epoxy. Heat curable. Exceptional abrasion and chemical resistance. Serviceable from -100°F to +450°F. Can withstand high compressive loads and rigorous thermal cycling. Good strength retention at elevated temperatures.

Two Part Epoxy System Supreme46HT-1AO Supreme 46HT-1AO

Toughened epoxy system, resists thermal cycling. Serviceable from -100°F to +500°F. Exceptionally long working life. Thermally conductive, electrically insulative.

Supreme 46HT-2 Two Part Epoxy Supreme 46HT-2

High strength epoxy adhesive. Outstanding toughness and durability. Serviceable from -100°F to +500°F. Withstand mechanical shocks and rigorous thermal cycling. Excellent peel strength. Cures at elevated temperature.

Supreme 46HT-2ND2 Two Component Epoxy Supreme 46HT-2ND2

Two component, non-drip, toughened, heat resistant epoxy adhesive. Superior durability and bond strength. Withstands chemical exposure. Paste consistency. Gap filling. Serviceable from -100°F to +500°F. Successfully tested for 1,000 hours 85°C/85% RH. Outstanding thermal cycling capabilities.

Supreme 46HTQ Two Component Epoxy Supreme 46HTQ

Quartz filled epoxy system for bonding, sealing, casting. Service temperature range -80°F to +500°F. Superior chemical and abrasion resistance. Dimensional stability. High compressive strength. Good strength retention at elevated temperatures. Oven curing compound.

Supreme 62-1 Two Part Epoxy Supreme 62-1

Cures rapidly at moderate elevated temperatures. Superior resistance to moisture. Two part epoxy has long pot life at ambient temperatures. High bond strength properties. Reliable electrical insulator. Serviceable from -60°F to +450°F. Withstands aggressive chemical exposure. Tg 160-165°C. Shore D hardnes >80. Excellent toughness.

Supreme 65HT-6 Two Part Epoxy Supreme 65HT-6

Fast room temperature curing heat resistant epoxy adhesive. Serviceable from -80°F to +400°F. Sets up in 5-10 minutes at room temperatures. High tensile lap shear strength. Superior dimensional stability. Good chemical resistance. Tough bonds. Ability to withstand impact and thermal cycling.

Supreme 70CN Two Part Epoxy Supreme 70CN

Two component, toughened epoxy system for bonding, sealing, coating and potting derived from natural substances. Low shrinkage upon curing. Exceptional wetting properties. Service temperature range is -100°F to +450°F.

UV10 One Part UV Curable Compound UV10

One component, no mix, UV curable adhesive. High strength bonds and superior chemical resistance properties. Low viscosity. Excellent dimensional stability. Fast curing. Serviceable from -60°F to +300°F.